PERMABOND TA4592

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND TA4592

Main features

  • External-Mix Automated Dispensing
  • Sub-30-Second Gel Time
  • Motor Magnet and Ferrite Bonding

Product Description

Permabond TA4592 is a two-component, 1:1 external-mix structural acrylic adhesive for bonding magnets and ferrites in electric motors. Part A and Part B are dispensed separately and mixed as the beads fall onto the part, supporting high-speed automated assembly without a static mixer. The system fills gaps up to 1 mm, gels in less than 30 seconds, fixtures zinc in 10-30 seconds, and cures fully in 24 hours. Typical cured performance includes 20-25 N/mm2 shear strength on mild steel, 15-20 N/mm2 on zinc, and 10-20 kJ/m2 impact strength.

Key features

  • External-Mix Automation: Two dispensed components mix in air without a static mixer.
  • Sub-30-Second Gel: A 1 g plus 1 g mix gels in less than 30 seconds.
  • Motor Magnet and Ferrite Bonding: Targets magnet and ferrite attachment in electric-motor assembly.

Applications

Applications include automated bonding of magnets and ferrites in electric motors and supported structural acrylic assemblies.

Product Family

PERMABOND TA4592

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Blue / Yellow-green
Component System
TA4592 A / TA4592 B
Mix Ratio
1:1
Other Properties
Maximum gap fill
1 mm
Storage Temperature
2 - 7 °C
Curing Conditions
Fixture Time
10-30 seconds
Thermal Properties
Thermal Conductivity
0.1 W/m.K

Additional Information

Technical properties

As supplied / before processing

Part A and Part B are shown separately; processing values apply to the stated 1:1 external-mix system.

Property Value Unit Method / condition
AppearancePart A: blue; Part B: yellow-greenAs supplied
Part A viscosity10,000-15,000; 40,000-60,000mPa s20 rpm; 2.5 rpm at 25 deg C
Part B viscosity5,000-6,000; 12,000-15,000mPa s20 rpm; 2.5 rpm at 25 deg C
DensityPart A: 1.1; Part B: 1.1As supplied
Mix ratio1:1External mix
Maximum gap fill1mmTypical curing property
Cure milestonesGel: <30 seconds; zinc fixture: 10-30 seconds; full cure: 24 hoursGel based on 1 g Part A plus 1 g Part B
Storage temperature2 to 7deg CRecommended storage range
Technical properties

After processing / final state

Values are typical for cured adhesive and the stated substrates, cure periods, and methods.

Property Value Unit Method / condition
Shear strength - mild steel20-25N/mm2Typical cured value
Shear strength - zinc15-20N/mm2Typical cured value
Shear strength - steel to ferrite, 3 minutes4N/mm2Typical cure development
Shear strength - steel to ferrite, 24 hours>14N/mm2Substrate failure
Tensile strength25N/mm2ASTM D2095
Impact strength10-20kJ/m2ASTM D-950
Coefficient of thermal expansion80 x 10^-61/KASTM D-696
Thermal conductivity0.1W/(m K)ASTM C-177