PERMABOND TA4590

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND TA4590

Main features

  • 15-30 Second Steel Fixture
  • 2-3 Minute Working Strength
  • Non-Corrosive Copper Bonding

Product Description

Permabond TA4590 is a blue, thixotropic no-mix structural acrylic adhesive used with Permabond Initiator 44. It bonds metals, ferrites, ceramics, and selected thermoplastics, with an acid-free formulation developed for sensitive copper parts and other conductive surfaces. The system fills gaps up to 0.5 mm, fixtures gap-free mild steel in 15-30 seconds at 23 deg C, and reaches working strength in 2-3 minutes. Typical 24-hour shear strength at 25 deg C is 20-25 N/mm2 on steel and greater than 14 N/mm2 on steel-to-ferrite assemblies, where substrate failure was reported.

Key features

  • 15-30 Second Fixture: Fixtures gap-free mild steel in 15-30 seconds with Initiator 44.
  • 2-3 Minute Working Strength: Develops working strength rapidly at 23 deg C.
  • Non-Corrosive Conductive-Surface Bonding: Acid-free formulation supports sensitive copper and conductive surfaces.

Applications

Applications include structural bonding of metals, ferrites, ceramics, selected thermoplastics, and sensitive conductive surfaces with Initiator 44.

Product Family

PERMABOND TA4590

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Blue, thixotropic
Mix Ratio
10:1.5 approximately
Specific Gravity
1.1
Physical Properties
Viscosity
15,000 – 25,000 mPa.s
Other Properties
Maximum gap fill
0.5 mm
Storage Temperature
5 - 25 °C
Curing Conditions
Fixture Time
15-30 seconds
Mechanical Properties
Peel Strength
85-100 N/25mm
Thermal Properties
Thermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric Strength
30-50 kV/mm
Volume Resistivity
2 x 10¹³ Ohms⋅cm

Additional Information

Technical properties

As supplied / before processing

Resin values are shown with processing values for use with Permabond Initiator 44.

Property Value Unit Method / condition
AppearanceBlue, thixotropicAs supplied
Viscosity15,000-25,000mPa s20 rpm at 25 deg C
Low-shear viscosity50,000-120,000mPa s2.5 rpm at 25 deg C
Specific gravity1.1Resin as supplied
Use ratioApprox. 10:1.5TA4590 adhesive to Initiator 44
Maximum gap fill0.5mmTypical curing property
Cure milestonesFixture: 15-30 seconds; handling: 30-60 seconds; working strength: 2-3 minutes; full cure: 24 hoursMild steel, no induced gap, at 23 deg C
Storage temperature5 to 25deg CRecommended storage range
Technical properties

After processing / final state

Values are typical for cured adhesive; strength depends on surface preparation, gap, cure, and substrate.

Property Value Unit Method / condition
Shear strength - steel20-25N/mm2ISO 4587; 24-hour cure at 25 deg C
Shear strength - steel to ferrite>14N/mm2ISO 4587; 24-hour cure at 25 deg C; substrate failure
Shear strength - zinc12-18N/mm2ISO 4587; 24-hour cure at 25 deg C
Peel strength - aluminum85-100N/25 mmISO 4578
Tensile strength20-30N/mm2ISO 37
Impact strength15-20kJ/m2ASTM D-950
Dielectric strength30-50kV/mmASTM D-149
Volume resistivity2 x 10^13ohm cmASTM D-257

Leading Brands Trust in Our Products and Services