PERMABOND TA459

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND TA459

Main features

  • 20-40 Second Steel Fixture
  • 20-25 N/mm2 Steel Shear
  • Non-Corrosive Copper Bonding

Product Description

Permabond TA459 is a no-mix toughened acrylic structural adhesive for bonding metals, ferrites, ceramics, and selected thermoplastics. It is used with Initiator 41 or 41M, or Initiator 43 for plastics, with the initiator applied to one surface and adhesive to the other. The thixotropic formulation fills gaps up to 0.5 mm, fixtures gap-free mild steel in 20-40 seconds at 23 deg C, and reaches working strength in 3-5 minutes. After 24 hours at 25 deg C, typical steel shear strength is 20-25 N/mm2. The acid-free formulation is non-corrosive to sensitive copper and conductive surfaces.

Key features

  • 20-40 Second Fixture: Fixtures gap-free mild steel in 20-40 seconds at 23 deg C.
  • No-Mix Initiator Process: Uses separate adhesive and initiator application without premixing.
  • Non-Corrosive Conductive-Surface Bonding: Acid-free formulation supports sensitive copper and conductive surfaces.

Applications

Applications include structural bonding of metals, ferrites, ceramics, selected thermoplastics, and sensitive conductive surfaces with the specified initiator.

Product Family

PERMABOND TA459

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Blue, thixotropic
Mix Ratio
10:1.5 approximately
Specific Gravity
1.1
Physical Properties
Viscosity
15,000 – 25,000 mPa.s
Other Properties
Maximum gap fill
0.5 mm
Storage Temperature
5 - 25 °C
Curing Conditions
Fixture Time
20-40 seconds
Mechanical Properties
Peel Strength
85-100 N/25mm
Thermal Properties
Thermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric Strength
30-50 kV/mm
Volume Resistivity
2 x 10¹³ Ohms⋅cm

Additional Information

Technical properties

As supplied / before processing

Resin values are shown with processing values for the specified Permabond initiator system.

Property Value Unit Method / condition
AppearanceBlue, thixotropicAs supplied
Viscosity15,000-25,000mPa s20 rpm at 25 deg C
Low-shear viscosity50,000-100,000mPa s2.5 rpm at 25 deg C
Specific gravity1.1Resin as supplied
Use ratioApprox. 10:1.5Adhesive to Initiator 41 or 41M
Maximum gap fill0.5mmTypical curing property
Cure milestonesFixture: 20-40 seconds; handling: 40-75 seconds; working strength: 3-5 minutes; full cure: 24 hoursMild steel, no gap, at 23 deg C
Storage temperature5 to 25deg CRecommended storage range
Technical properties

After processing / final state

Values are typical for cured adhesive; strength depends on surface preparation, gap, cure, and substrate.

Property Value Unit Method / condition
Shear strength - steel20-25N/mm2ISO 4587; 24-hour cure at 25 deg C
Shear strength - steel to ferrite>14N/mm2ISO 4587; 24-hour cure at 25 deg C; substrate failure
Shear strength - zinc12-18N/mm2ISO 4587; 24-hour cure at 25 deg C
Peel strength - aluminum85-100N/25 mmISO 4578
Tensile strength20-30N/mm2ISO 37
Impact strength15-20kJ/m2ASTM D-950
Dielectric strength30-50kV/mmASTM D-149
Volume resistivity2 x 10^13ohm cmASTM D-257