PERMABOND TA4246

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND TA4246

Main features

  • 1-2 Minute Aluminum Fixture
  • 33-35 N/mm2 Steel Shear
  • No-Mix Initiator 46 System

Product Description

Permabond TA4246 is a two-part, no-mix toughened acrylic structural adhesive used with Permabond Initiator 46. The adhesive is applied to one surface and the initiator to the other, eliminating premixing while supporting room-temperature assembly. It fills gaps up to 0.5 mm, fixtures aluminum in 1-2 minutes at 23 deg C, and reaches working strength in 15-30 minutes. After a 24-hour cure, typical shear strength is 33-35 N/mm2 on mild steel and 20-30 N/mm2 on aluminum, with 150-180 N/25 mm peel strength. Applications include structural bonding across supported metals, plastics, ceramics, and other substrates.

Key features

  • No-Mix Structural Bonding: Separate adhesive and Initiator 46 application eliminates premixing.
  • 1-2 Minute Aluminum Fixture: Fixtures gap-free aluminum in 1-2 minutes at 23 deg C.
  • High Shear and Peel: Provides 33-35 N/mm2 steel shear and 150-180 N/25 mm aluminum peel strength.

Applications

Applications include structural bonding of supported metals, plastics, ceramics, wood, glass, and composite materials.

Product Family

PERMABOND TA4246

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Amber liquid
Mix Ratio
10:1 approximately
Specific Gravity
1.0
Physical Properties
Viscosity
15,000 – 35,000 mPa.s
Other Properties
Maximum gap fill
0.5 mm
Storage Temperature
2 - 7 °C
Curing Conditions
Fixture Time
1-2 minutes
Mechanical Properties
Peel Strength
150-180 N/25mm
Thermal Properties
Thermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric Strength
30-50 kV/mm
Volume Resistivity
2 x 10¹³ Ohms⋅cm

Additional Information

Technical properties

As supplied / before processing

Resin values are shown with processing values for use with Permabond Initiator 46.

Property Value Unit Method / condition
AppearanceAmber liquidAs supplied
Viscosity15,000-35,000mPa s20 rpm at 25 deg C
Specific gravity1.0Resin as supplied
Use ratioApprox. 10:1TA4246 adhesive to Initiator 46
Maximum gap fill0.5mmTypical curing property
Cure milestonesFixture: 1-2; handling: 2-4; working strength: 15-30minutesAluminum, no gap, at 23 deg C
Full cure24hoursAt 23 deg C
Storage temperature2 to 7deg CRecommended storage range
Technical properties

After processing / final state

Values are typical for fully cured adhesive; strength depends on surface preparation and bond gap.

Property Value Unit Method / condition
Shear strength - mild steel33-35N/mm2ISO 4587
Shear strength - aluminum20-30N/mm2ISO 4587
Peel strength - aluminum150-180N/25 mmISO 4578
Tensile strength30N/mm2ISO 37
Impact strength50-60kJ/m2ASTM D-950
Coefficient of thermal expansion80 x 10^-61/KASTM D-696
Thermal conductivity0.1W/(m K)ASTM C-177