PERMABOND QFS16

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND QFS16

Main features

  • 5-Second Steel Set Time
  • Faster Cure Through Gaps
  • Reduced Plastic Stress Cracking

Product Description

Permabond QFS16 is a colorless cyanoacrylate activator for shortening set time on closely mated parts, porous surfaces, gaps, and wire-tacking assemblies. It is applied to one component by wiping, spraying, or dipping and allowed to evaporate before adhesive is placed on the untreated surface. With a 100 cP ethyl-2-cyanoacrylate at 23 deg C, typical set time is 5 seconds on gap-free steel and 40-60 seconds across a 5 mil gap. The formulation also reduces stress cracking, surface discoloration, and adhesive frosting on supported plastic parts.

Key features

  • Rapid Steel Set: Provides a typical 5-second set on gap-free steel under stated conditions.
  • Gap and Porous-Surface Cure: Accelerates cyanoacrylate cure through gaps and on porous materials.
  • Reduced Plastic Surface Effects: Helps limit stress cracking, discoloration, and frosting on supported plastics.

Applications

Applications include porous or poorly mated parts, gap bonding, wire tacking, excess-fillet cure, and supported plastic assemblies.

Product Family

PERMABOND QFS16

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Colorless
Specific Gravity
0.68
Thermal Properties
Flash Point
-2 °C
Other Properties
Storage Temperature
5 - 25 °C

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Product typeCyanoacrylate activatorAs supplied
ColorColorlessAs supplied
Specific gravity0.68As supplied
Flash point-2deg CAs supplied
Application methodWipe, spray, or dip one componentAllow full evaporation before bonding
Storage temperature5 to 25deg CRecommended storage range
Technical properties

After processing / final state

Set-time values apply to 100 cP ethyl-2-cyanoacrylate at 23 deg C; the control row is identified separately.

Property Value Unit Method / condition
Set time - steel, no gap5secondsAt 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS16
Set time - steel, 5 mil gap40-60secondsAt 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS16
Set time - steel, no gap, control10-15secondsAt 23 deg C without QFS16
Set time - Buna-N, no gap10secondsAt 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS16
Set time - phenolic, no gap5secondsAt 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS16

Leading Brands Trust in Our Products and Services