PERMABOND PT328

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PERMABOND PT328

Main features

  • 15-20 Minute Pot Life
  • 5 mm Gap Filling
  • 12-18 MPa Steel Shear

Product Description

Permabond PT328 is a two-part, room-temperature-curing polyurethane adhesive for bonding metals, plastics, and composites. Its 1:1 mix ratio and 15-20 minute pot life provide time for large-area assembly, while the thixotropic, non-slump rheology supports controlled placement. The material fills gaps up to 5 mm and reaches handling strength on steel in 90-120 minutes at 23 deg C. After cure, it provides 12-18 MPa shear strength on steel together with documented impact and vibration resistance. Applications include large bonded assemblies that require broad substrate coverage and an extended processing window.

Key features

  • Large-Area Work Window: Provides a 15-20 minute pot life for extended assembly operations.
  • 5 mm Gap Fill: Fills bond gaps up to 5 mm with a 1:1 mix ratio.
  • Impact and Vibration Resistance: Cured polyurethane supports assemblies exposed to impact and vibration.

Applications

Applications include large-area bonding of metals, plastics, and composites, including assemblies exposed to impact or vibration.

Product Family

PERMABOND PT328

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Black / Cream
Component System
Two (Polyurethane / Isocyanate)
Mix Ratio
1 : 1 by volume
Pot Life
15-20 minutes
Specific Gravity
1.25 / 1.45
Other Properties
Maximum gap fill
5 mm
Storage Temperature
5-25 °C
Mechanical Properties
Elongation
<20 %

Additional Information

Technical properties

As supplied / before processing

Part A and Part B values are shown separately; processing values apply after the stated 1:1 mix ratio.

Property Value Unit Method / condition
AppearancePart A: black; Part B: creamAs supplied
Part A viscosity4,000-8,000mPa sAt 25 deg C; thixotropic
Part B viscosity3,000-6,000mPa sAt 25 deg C; thixotropic
Specific gravityPart A: 1.25; Part B: 1.45As supplied
Mix ratio1:1By volume
Maximum gap fill5mmTypical curing property
Pot life15-20minutesTypical processing window
Full cure4-5 days; 30 minutesAt 23 deg C; at 90 deg C
Technical properties

After processing / final state

Values are typical for cured adhesive; strength varies with surface preparation and bond gap.

Property Value Unit Method / condition
Shear strength - steel12-18MPaISO 4587
Shear strength - zinc5-6MPaISO 4587
Shear strength - FRP glass epoxy5-7N/mm2ISO 4587
Shear strength - FRP glass polyester12-14N/mm2ISO 4587
Shear strength - carbon fiber9-11N/mm2ISO 4587
Tensile strength15-20MPaISO 37
Elongation at break<20%ISO 37
Hardness60-75Shore DISO 868