PERMABOND MT382

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PERMABOND MT382

Main features

  • Self-Leveling Electronic Potting
  • Extended 20-50 Minute Pot Life
  • High-Elongation Modified Epoxy

Product Description

Permabond MT382 is a two-part, self-leveling modified epoxy adhesive for sealing, bonding, electronic potting, and encapsulation. The system mixes 2:1 by volume and combines a 20-50 minute pot life at 25 deg C with a 105-120 minute handling time. Part A is a black epoxy resin and Part B is a yellow polyamine hardener, producing a charcoal-black mixed material. The cured epoxy provides 150-200% elongation, 140-160 N/25 mm peel strength on aluminum, and 0.47 W/(m K) thermal conductivity. Applications include nylon, ABS, polycarbonate, other supported plastics, and metal assemblies.

Key features

  • Self-Leveling Potting: Flows for electronic potting, encapsulation, sealing, and bonding.
  • Extended Processing Window: Provides a 20-50 minute pot life at 25 deg C.
  • Flexible Cured Epoxy: Provides 150-200% elongation with 140-160 N/25 mm aluminum peel strength.

Applications

Applications include electronic potting and encapsulation, sealing, and bonding of nylon, ABS, polycarbonate, other supported plastics, and metal assemblies.

Product Family

PERMABOND MT382

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Black / Yellow
Component System
Two (Epoxy Resin / Polyamine based Hardener)
Mix Ratio
2:1 by volume
Pot Life
20-50 minutes
Other Properties
Maximum gap fill
0.5 mm
Electrical Properties
Dielectric Strength
20 - 30 kV/mm
Volume Resistivity
1 - 3 x 10¹¹ Ohms⋅cm
Mechanical Properties
Elongation
150 -200 %
Peel Strength
140-160 N/25mm
Thermal Properties
Thermal Conductivity
0.47 W/m.K

Additional Information

Technical properties

As supplied / before processing

Part A and Part B values are shown separately; processing values apply after the stated mix ratio.

Property Value Unit Method / condition
Part A viscosity32,000mPa sAt 25 deg C
Part B viscosity300mPa sAt 25 deg C
Specific gravityPart A: 1.3; Part B: 1.0As supplied
Mix ratio2:1; 130:50By volume; by weight
Maximum gap fill0.5mmTypical curing property
Usable / pot life20-50minutesAt 25 deg C
Handling time105-120minutesTo 0.1 N/mm2 at 25 deg C
Full cure>=72hoursAt 25 deg C
Technical properties

After processing / final state

Property Value Unit Method / condition
Hardness55-85 Shore A; 20-30 Shore DISO 868
Elongation at break150-200%ISO 37
Peel strength - aluminum140-160N/25 mmISO 4578
Thermal conductivity0.47W/(m K)Typical cured value
Coefficient of thermal expansion112 x 10^-6; 170 x 10^-6m/m/deg CBelow Tg; above Tg
Glass transition temperature, Tg-35deg CTypical cured value