PERMABOND MS359

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

PERMABOND MS359

Main features

  • No-Mix Moisture Cure
  • 10-20 Minute Skin Formation
  • High-Elongation Exterior Bonding

Product Description

Permabond MS359 Grey is a single-part, moisture-curing MS polymer adhesive for exterior bonding and sealing. Its grey, high-viscosity formulation requires no mixing and develops a skin in 10-20 minutes, with an approximate cure rate of 5 mm per 24 hours. The cured material combines 45-60 Shore A hardness with 150-350% elongation for an elastomeric bond on supported metals, plastics, composites, PVC, polycarbonate, polystyrene, and wood. The adhesive is primer-free on supported substrates and can be painted after cure. Applications include exterior frames, fascias, and related construction assemblies.

Key features

  • No-Mix Moisture Cure: Single-part MS polymer cures by humidity without component mixing.
  • Controlled Skin Formation: Develops a skin in 10-20 minutes before continued cure.
  • Flexible Cured Bond: Provides 150-350% elongation and 45-60 Shore A hardness.

Applications

Applications include exterior construction bonding and sealing for frames and fascias, plus supported assemblies using metals, plastics, composites, PVC, polycarbonate, polystyrene, or wood.

Product Family

PERMABOND MS359

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Grey
Specific Gravity
1.5
Physical Properties
Viscosity
1,500,000-2,500,000 mPa.s
Mechanical Properties
Elongation
150-350 %
Other Properties
Storage Temperature
5-25 °C

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Chemical compositionMS polymerAs supplied
AppearanceGreyAs supplied
Viscosity1,500,000-2,500,000mPa s5 rpm at 25 deg C
Low-shear viscosity4,500,000-9,000,000mPa s1 rpm at 25 deg C
Specific gravity1.5As supplied
Curing mechanismHumidityRoom-temperature moisture cure
Skin-over time10-20minutesTypical curing property
Cure rateApprox. 5mm/24 hoursTypical curing property
Technical properties

After processing / final state

Property Value Unit Method / condition
Shear strength - steel, aluminum, zinc, PVC, or wood2-3MPaISO 4587
Shear strength - polycarbonate or polystyrene1-1.5MPaISO 4587
Tensile strength2-3MPaISO 37
Elongation at break150-350%ISO 37
Hardness45-60Shore AISO 868