PERMABOND LM113

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND LM113

Main features

  • Low-Strength Easy-Disassembly Threadlocking
  • Medium-Viscosity Non-Drip Application
  • MIL-S-46163A/ASTM D5363 Compliance

Product Description

Permabond® LM113 is a medium-viscosity, low-strength anaerobic threadlocker specifically designed for securing small threaded fasteners, screws, bolts, and hydraulic fittings that may require future disassembly. Formulated as a PFAS-free, 100% solid liquid, it cures rapidly at room temperature when confined between metal parts, providing excellent protection against vibration-induced loosening. Its thixotropic properties ensure the adhesive remains precisely where applied without running, while also lubricating the threads to facilitate easier initial assembly.

Key features

  • Low strength for disassembly: Provides a controlled off-torque (Breakaway 9 N-m), allowing for easy maintenance and disassembly of small or delicate fasteners.
  • Thixotropic rheology: The medium viscosity (1,200 cP) and thixotropic nature prevent the adhesive from dripping or migrating away from the application area.
  • Military and ASTM approved: Meets the strict lot testing requirements of military specification MIL-S-46163A (Type II Grade M) and ASTM D5363 (AN 0311 Group 03 Class 1 Grade 1).

Applications / Suitable for

  • Locking and sealing small threaded fasteners, screws, bolts, and hydraulic fittings (up to M20 / 3/4")
  • Assemblies requiring protection against vibration loosening and corrosion
  • Applications requiring controlled, low-strength locking for future disassembly and maintenance
Product Family

PERMABOND LM113

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Purple
Chemistry Type
Methacrylate esters
Specific Gravity
1.1
Physical Properties
Viscosity
1,200 mPa.s
Other Properties
Maximum gap fill
0.15 mm
Maximum thread size
M20 ¾"
Electrical Properties
Dielectric Strength
11 kV/mm
Thermal Properties
Thermal Conductivity
0.19 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Methacrylate esters - -
Appearance Purple / Violet - Liquid
Viscosity 1,200 mPa.s (cP) at 25°C (Thixotropic)
Specific Gravity 1.1 - -
Maximum Gap Fill 0.15 mm (0.006 in)
Maximum Thread Size M20 - (3/4")
Flash Point > 100 °C (212°F)
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Handling Strength Time 15 minutes M10 steel at 23°C
Full Strength Time 24 hours M10 steel at 23°C
Breakaway Torque Strength 9 N-m M10 steel (ISO 10964) (80 in.lb)
Prevailing Torque Strength 5 N-m M10 steel (ISO 10964) (40 in.lb)
Shear Strength 5 MPa Steel collar & pin (ISO 10123) (750 psi)
Coefficient of Thermal Expansion 90E-6 mm/mm/°C -
Dielectric Strength 11 kV/mm -
Thermal Conductivity 0.19 W/(m.K) -