PERMABOND LH050

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND LH050

Main features

  • Up to 1000 psi Instant Air Seal
  • PTFE Non-Shredding Pipe-Dope Alternative
  • UL Gas/Fuel/Sprinkler Classification

Product Description

Permabond® LH050 is a general-purpose, PTFE-filled anaerobic pipe sealant that cures to form a solid plastic seal when confined between threaded metal parts. Formulated as a smooth white paste, it immediately provides an air pressure seal up to 1000 psi with only limited hand tightening, and upon full cure, its sealing capability matches the burst rating of the pipe itself. Its low locking strength facilitates easy disassembly, making it an excellent, non-shredding alternative to traditional pipe dopes and PTFE tapes.

Key features

  • Instant seal capability: Delivers an immediate air pressure seal up to 1000 psi upon application, prior to full cure.
  • UL Classified: Classified by Underwriters Laboratories (UL) for use in systems handling gasoline, petroleum oils, natural gas, propane, and butane, as well as sprinkler and water spray systems.
  • Reliable & Clean: 100% solid, solvent-free formulation that will not shred, tear, or cause blockages in fine filters or valves like traditional PTFE tape can.

Applications / Suitable for

  • Sealing threaded metallic pipe joints, plugs, and fittings (particularly steel and brass)
  • Systems requiring UL classification for handling fuels, oils, or gases
  • Assemblies requiring an instant pressure seal and easy subsequent disassembly
Product Family

PERMABOND LH050

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
White
Chemistry Type
Methacrylate esters
Specific Gravity
1.1
Physical Properties
Viscosity
250,000 mPa.s
Other Properties
Maximum gap fill
0.5 mm
Thermal Properties
Thermal Conductivity
0.19 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Methacrylate esters - -
Appearance White - Paste
Viscosity 250,000 mPa.s (cP) at 23°C - 25°C
Specific Gravity 1.1 - -
Maximum Gap Fill 0.5 mm (0.02 in)
Particle Size < 10 µm -
Flash Point > 100 °C -
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Handling Strength Time 2 hours M10 steel at 23°C
Full Strength Time 24 hours M10 steel at 23°C
Breakaway Torque Strength 4 N-m M10 steel (ISO 10964) (35 in.lb)
Prevailing Torque Strength 3 N-m M10 steel (ISO 10964) (25 in.lb)
Compressive Shear Strength 7 MPa Steel collar & pin (ISO 10123) (1000 psi)
Coefficient of Thermal Expansion 90E-6 mm/m/°K -
Coefficient of Thermal Conductivity 0.19 W/(m.K) -

Leading Brands Trust in Our Products and Services