PERMABOND HM-162

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND HM-162

Main features

  • 5-Minute Steel Handling Time
  • 30 MPa Shear Strength
  • High-Temperature Chemical Resistance

Product Description

Permabond® HM162 is a medium-viscosity anaerobic retaining compound that cures rapidly when confined between close-fitting metal parts. Engineered to form an extremely tough bond, it excels in applications involving cylindrical parts where very high strength and improved fatigue life are paramount. In its uncured state, the liquid adhesive wets out metal surfaces perfectly, keying into surface irregularities and effectively filling the space between mated components.

Key features

  • Rapid curing: Achieves handling strength on steel in just 5 minutes at room temperature, significantly accelerating assembly processes.
  • Superior performance: Delivers very high shear strength (30 MPa) and improved fatigue life, ensuring durable bonds under high stress.
  • High temperature resistance: Specially formulated to maintain excellent bond strength and integrity in elevated temperature environments.

Applications / Suitable for

  • Retaining and sealing cylindrical metal parts (up to 0.2 mm gap)
  • Assemblies requiring improved fatigue life and high shear strength
  • Applications operating in high-temperature or chemically harsh environments
Product Family

PERMABOND HM-162

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Green
Chemistry Type
Acrylic
Specific Gravity
1.1
Physical Properties
Viscosity
1,000 mPa.s
Other Properties
Maximum gap fill
0.2 mm
Maximum thread size
M20 ¾
Electrical Properties
Dielectric Strength
11 kV/mm
Thermal Properties
Thermal Conductivity
0.19 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Acrylic - -
Appearance Green - Liquid
Viscosity ~ 1,000 mPa.s (cP) at 23°C - 25°C
Specific Gravity 1.1 - -
Maximum Gap Fill 0.2 mm (0.008")
UV Fluorescence Yes - -
Flash Point > 100 °C -
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Handling Strength Time 5 minutes M10 steel at 23°C
Working Strength Time 1-3 hours M10 steel at 23°C
Full Strength Time 24 hours M10 steel at 23°C
Breakaway Torque Strength 32 N-m M10 steel (ISO 10964) (280 in.lb)
Prevailing Torque Strength 57 N-m M10 steel (ISO 10964) (510 in.lb)
Shear Strength 30 MPa Steel collar & pin (ISO 10123) (4300 psi)
Coefficient of Thermal Expansion 90E-6 mm/m/°C -
Dielectric Strength 11 kV/mm -