PERMABOND HH120

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND HH120

Main features

  • High-Viscosity Non-Drip Threadlocking
  • MIL-S-46163A/MIL-S-22473E/ASTM D5363 Compliance
  • Vibration/Corrosion-Resistant Thread Retention

Product Description

Permabond® HH120 is an excellent general-purpose anaerobic threadlocker and sealant designed for the permanent assembly of bolts, nuts, and screws. Featuring a high-viscosity, non-drip, and thixotropic formulation, it is particularly well-suited for coarse threaded fasteners where precise application without slumping is required. It cures fast and reliably at room temperature on various metal surfaces, including steel, cadmium, zinc, and other plated fasteners, providing exceptional environmental and corrosion resistance.

Key features

  • Military and Industry specified: Tested to meet the strict requirements of MIL-S-46163A, MIL-S-22473E, and ASTM D5363 standards.
  • High viscosity & Non-drip: The 7,000 cP thixotropic formulation ensures the adhesive stays in place, making it ideal for coarse threads and blind holes.
  • Vibration and corrosion protection: Reliably prevents vibration loosening while providing a 100% solid, environmentally friendly barrier against corrosion.

Applications / Suitable for

  • Permanent locking of coarse threaded fasteners, bolts, nuts, and screws
  • Sealing pipe flanges and retaining worn bearings
  • Machinery and equipment manufacturing
Product Family

PERMABOND HH120

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Red
Chemistry Type
Methacrylate esters
Specific Gravity
1.2
Work life @25°C
0.5 hours
Physical Properties
Viscosity
7,000 mPa.s
Other Properties
Maximum gap fill
0.25 mm mm
Electrical Properties
Dielectric Strength
11 kV/mm
Thermal Properties
Thermal Conductivity
0.19 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Methacrylate esters - -
Appearance Red - Liquid
Viscosity ~ 7,000 cP / mPa.s at 25°C
Specific Gravity 1.1 - -
Maximum Gap Fill 0.25 mm (0.01 in)
Maximum Thread Size M30 - (1 1/4")
UV Fluorescence Yes - -
Flash Point > 100 °C -
Volatile Organic Compound < 2 % 20 grams/liter (Estimated)
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Handling Strength Time 10 minutes M10 steel at 23°C
Working Strength Time 30 minutes M10 steel at 23°C
Full Strength Time 24 hours M10 steel at 23°C
Breakaway Torque Strength 31 N-m M10 steel (ISO 10964) (275 in.lb)
Prevailing Torque Strength 34 N-m M10 steel (ISO 10964) (300 in.lb)
Shear Strength 17 MPa Steel collar & pin (ISO 10123) (2500 psi)
Coefficient of Thermal Expansion 90E-6 mm/m/°C -
Dielectric Strength 11 kV/mm -
Thermal Conductivity 0.19 W/(m.K) -