PERMABOND ET5422

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PERMABOND ET5422

Main features

  • Impact and Vibration Resistance
  • Up to 5 mm Gap Filling
  • Elevated-Temperature Bond Strength

Product Description

Permabond® ET5422 is a high-performance, two-part epoxy adhesive formulated specifically for applications demanding exceptional toughness and high structural strength. This 2:1 mixable system features controlled-flow, thixotropic properties, making it highly effective for gap-filling applications while ensuring ease of mixing and application. It delivers excellent resistance to impact, vibration, and elevated temperatures, providing durable bonds across metals and composite materials.

Key features

  • Exceptional toughness: Formulated to provide maximum impact and vibration resistance for highly stressed structural joints.
  • Thixotropic rheology: Controlled flow characteristics allow the adhesive to be easily applied while remaining suitable for gap-filling applications up to 5 mm.
  • High temperature performance: Delivers exceptional bond strength even at elevated temperatures, which can be further improved with a brief post-cure cycle.

Applications / Suitable for

  • Structural bonding of metals (steel, aluminum, galvanized) and composites (carbon fiber, GFRP)
  • Assemblies requiring high impact and vibration resistance
  • Applications requiring controlled flow for gap filling or vertical application
Product Family

PERMABOND ET5422

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
A:Epoxy Resin/B:Modified Polyamide
Mix Ratio
2:1 by volume 100:44 by weight
Pot Life
180 minutes
Solids
100 %
Specific Gravity
A:1.14/ B:1.0
Work life @25°C
24 hours
Physical Properties
Viscosity (Part A)
105,000 mPa.s
Viscosity (Part B)
100,000 mPa.s
Mechanical Properties
Impact Strength
20-30 KJ/m² mm
Peel Strength
Cured 1hr @ 60°C: 270 N/25mm / Cured 5 days @ 23°C: 320 N/25mm
Thermal Properties
Glass Transition Temperature (Tg)
5d @ 23°C: 60°C/ 3d @ 23°C + 60min @ 80°C: 115°C °C
Other Properties
Maximum gap fill
5 mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Mix Ratio by Volume 2:1 - -
Mix Ratio by Weight 100:44 - -
Chemical Composition Epoxy Resin - Part A (A-side)
Chemical Composition Modified Polyamide - Part B (B-side)
Appearance Off White - Part A (A-side)
Appearance Blue - Part B (B-side)
Viscosity (Part A) 105,000 cP at 25°C, 20rpm (Thixotropic) (mPa.s)
Viscosity (Part B) 100,000 cP at 25°C, 20rpm (Thixotropic) (mPa.s)
Specific Gravity (Part A) 1.14 - -
Specific Gravity (Part B) 1.00 - -
Maximum Gap Fill 5 mm (0.2 in)
Flash Point > 100 °C -
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Usable / Pot Life 3 hours at 23°C (10g)
Usable / Pot Life 1 hour at 23°C (200g)
Handling Time 16 hours at 23°C
Working Strength 24 hours at 23°C
Full Cure 5 days at 23°C
Full Cure 1 hour at 80°C
Shear Strength 30-40 N/mm² Aluminium (ISO 4587) (4350-5800 psi)
Shear Strength 30-38 N/mm² Mild Steel (ISO 4587) (4350-5510 psi)
Shear Strength 20-26 N/mm² Stainless Steel (ISO 4587) (2900-3770 psi)
Shear Strength 18-24 N/mm² Hot Dip Galv (ISO 4587) (2610-3480 psi)
Shear Strength > 22 N/mm² Carbon Fibre (ISO 4587) (>3190 psi) SF
Shear Strength > 20 N/mm² Epoxy GFRP (ISO 4587) (>2900 psi) SF
Shear Strength > 10 N/mm² Polyester GRP (ISO 4587) (>1450 psi) SF
Peel Strength 270 N/25mm Aluminium (ISO 4578) Cured 1hr @ 60°C (59 PIW)
Peel Strength 320 N/25mm Aluminium (ISO 4578) Cured 5 days @ 23°C (70 PIW)
Impact Strength 20-30 KJ/m² ASTM D-950
Hardness > 80 Shore D ISO 868
Glass Transition Temperature (Tg) 60 °C DSC, 5d @ 23°C (140°F)
Glass Transition Temperature (Tg) 115 °C DSC, 3d @ 23°C + 60min @ 80°C (239°F)