Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PERMABOND ET540

Main features

  • Toughened Epoxy Bonding
  • 120 to 150-Minute Working Window
  • Metal-to-Wood Epoxy Bonding

Product Description

Permabond® ET540 is a two-part, 2:1 mixable, semi-flexible toughened epoxy adhesive designed to deliver high peel resistance and high shear strength. Formulated with a no-slump, non-drip rheology, it is highly suitable for large gaps and vertical applications across a variety of substrates including wood, metal, ceramics, and many plastics and composites. It offers an extended work life, making it ideal for larger applications that require adjustments during assembly.

Key features

  • Non-drip rheology: The thixotropic, no-slump nature of the mixed adhesive makes it perfect for filling large gaps (up to 5 mm) and for use on vertical surfaces without running.
  • Extended pot life: Offers a long usable life of 120-150 minutes, providing ample time for the assembly and adjustment of large components.
  • High structural strength: Toughened and semi-flexible, it provides excellent impact strength, high peel resistance, and high shear strength across diverse substrates while resisting high temperatures.

Applications / Suitable for

  • Large-scale assemblies requiring an extended working time for adjustments
  • Vertical applications or assemblies with large gaps (up to 5 mm) requiring a non-slump adhesive
  • Structural bonding of metals, wood, ceramics, plastics, and composites
Product Family

PERMABOND ET540

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
A:Epoxy Resin/B:Polyamine Hardener
Mix Ratio
2:1
Pot Life
120-150 minutes
Solids
100 %
Specific Gravity
A:1.1/ B:1.0
Work life @25°C
24 hours
Physical Properties
Viscosity (Part A)
75,000 mPa.s
Viscosity (Part B)
150,000 mPa.s
Mechanical Properties
Elongation
4-8 %
Peel Strength
60-80 N/25mm
Thermal Properties
Glass Transition Temperature (Tg)
45-55 °C
Thermal Conductivity
0.55 W/m.K
Electrical Properties
Dielectric Strength
15-25 kV/mm
Other Properties
Maximum gap fill
5 mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Mix Ratio by Volume 2:1 - -
Chemical Composition Epoxy Resin - Part A (ET540 A)
Chemical Composition Polyamine Hardener - Part B (ET540 B)
Appearance White - Part A
Appearance Amber - Part B
Viscosity (Part A) 75,000 cP at 25°C, 20rpm (mPa.s)
Viscosity (Part A) 225,000 cP at 25°C, 2rpm (mPa.s)
Viscosity (Part B) 150,000 cP at 25°C, 20rpm (mPa.s)
Viscosity (Part B) 500,000 cP at 25°C, 2rpm (mPa.s)
Specific Gravity (Part A) 1.1 - -
Specific Gravity (Part B) 1.0 - -
Maximum Gap Fill 5 mm (0.2 in)
Usable / Pot Life 120-150 minutes at 23°C
Flash Point > 100 °C -
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Handling Time 150-180 minutes at 23°C
Working Strength 24 hours at 23°C
Full Cure 72 hours at 23°C
Shear Strength 22-26 N/mm² Mild steel (ISO 4587) (3190-3770 psi)
Shear Strength 20-24 N/mm² Aluminium (ISO 4587) (2900-3480 psi)
Shear Strength 32-35 N/mm² Stainless Steel (ISO 4587) (4640-5075 psi)
Shear Strength > 25 N/mm² Carbon Fibre (ISO 4587) (>3625 psi) SF
Shear Strength > 8 N/mm² FRP Glass/Polyester (ISO 4587) (>1160 psi) SF
Shear Strength 23-27 N/mm² FRP Glass/Epoxy (ISO 4587) (3335-3915 psi)
Shear Strength 2-3 N/mm² PEEK (ISO 4587) (290-435 psi)
Shear Strength 2-4 N/mm² Polycarbonate (ISO 4587) (290-580 psi)
Shear Strength 3-5 N/mm² PA6 30% filled (ISO 4587) (435-725 psi)
Peel Strength 60-80 N/25mm Aluminium (ISO 11339) (13-18 PIW)
Hardness 60-75 Shore D ISO 868
Elongation at Break 4-8 % ISO 37
Glass Transition Temperature (Tg) 45-55 °C (113-131°F)
Dielectric Strength 15-25 kV/mm -
Thermal Conductivity 0.55 W/(m.K) -