PERMABOND ET515

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PERMABOND ET515

Main features

  • Flexible Cured Adhesive
  • 10 to 20-Minute Working Window
  • Up to 2 mm Gap Filling

Product Description

Permabond® ET515 Two-Part Epoxy is a 1:1 mixable, semi-flexible toughened epoxy adhesive. It cures relatively fast at room temperature, reaching handling strength in just 20-30 minutes, and provides excellent adhesion to a diverse array of substrates including wood, metal, ceramics, plastics, and composites. Its semi-flexible nature provides good impact strength and makes it highly suitable for bonding dissimilar materials where differential thermal expansion is anticipated.

Key features

  • Semi-flexible and toughened: Provides good impact strength and flexibility, accommodating differential thermal expansion between dissimilar bonded materials.
  • Fast room-temperature cure: A relatively fast-curing epoxy that achieves handling strength in 20-30 minutes without the need for external heat.
  • Versatile adhesion: Bonds strongly to a wide variety of substrates including metals, wood, ceramics, composites, and certain plastics.

Applications / Suitable for

  • Bonding dissimilar materials subject to thermal cycling or expansion
  • Structural bonding of wood, metal, ceramics, and composites
  • Assemblies requiring a semi-flexible, impact-resistant joint
Product Family

PERMABOND ET515

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Colourless
Chemistry Type
A:Epoxy Resin/B:Polyamine Hardener
Mix Ratio
1:1
Pot Life
10 - 20 minutes
Solids
100 %
Specific Gravity
A:1.1/ B:1.1
Physical Properties
Viscosity (Part A)
15,000 mPa.s mPa.s
Viscosity (Part B)
19,000 mPa.s
Mechanical Properties
Elongation
20-40 %
Peel Strength
100-150 N/25mm
Thermal Properties
Glass Transition Temperature (Tg)
20 °C
Thermal Conductivity
0.34 W/m.K
Electrical Properties
Dielectric Strength
15-25 kV/mm
Other Properties
Maximum gap fill
2 mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Mix Ratio by Volume 1:1 - -
Chemical Composition Epoxy Resin - Part A
Chemical Composition Polyamine Hardener - Part B
Appearance Colourless - Part A (Liquid)
Appearance Colourless - Part B (Liquid)
Viscosity (Part A) 15,000 cP at 25°C, 20rpm
Viscosity (Part B) 19,000 cP at 25°C, 20rpm
Specific Gravity 1.1 - Part A and Part B
Maximum Gap Fill 2 mm (0.08 in)
Flash Point > 100 °C -
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Usable / Pot Life 10-20 minutes at 23°C
Handling Time 20-30 minutes at 23°C
Working Strength 24 hours at 23°C
Full Cure 72 hours at 23°C
Shear Strength 8-12 N/mm² Mild steel (ISO 4587) (1160-1740 psi)
Shear Strength 9-12 N/mm² Aluminium (ISO 4587) (1305-1740 psi)
Shear Strength 6-9 N/mm² Stainless Steel (ISO 4587) (870-1305 psi)
Shear Strength 3-12 N/mm² Carbon Fibre (ISO 4587) (1160-1740 psi)
Shear Strength 3-5 N/mm² FRP Glass/Polyester (ISO 4587) (435-725 psi)
Shear Strength 4-6 N/mm² FRP Glass/Epoxy (ISO 4587) (580-870 psi)
Shear Strength > 5 N/mm² Polycarbonate (ISO 4587) (>725 psi) SF
Shear Strength 4-5 N/mm² PA6 30% filled (ISO 4587) (580-725 psi)
Peel Strength 100-150 N/25mm Aluminium (ISO 11339) (23-34 PIW)
Hardness 30-50 Shore D ISO 868
Elongation at Break 20-40 % ISO 37
Glass Transition Temperature (Tg) 20 °C (68°F)
Dielectric Strength 15-25 kV/mm -
Thermal Conductivity 0.34 W/(m.K) -

Leading Brands Trust in Our Products and Services