PERMABOND ET5147

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

PERMABOND ET5147

Main features

  • 2 mm Structural Gap Filling
  • Extended 40-60 Minute Pot Life
  • FDA 175.105 Formulation

Product Description

Permabond ET5147 is a two-part, 2:1 epoxy adhesive for structural bonding of metal, wood, composites, and certain plastics. Its controlled-flow formulation fills gaps up to 2 mm, while a 40-60 minute pot life at 23 deg C provides assembly time before handling strength develops in 3-5 hours. Full cure is reached in 72 hours at 23 deg C or 1 hour at 60 deg C. Typical cured performance includes 18-20 N/mm2 shear strength on mild steel and 40-70 N/25 mm peel strength on aluminum. The formulation is made to meet FDA 175.105 requirements.

Key features

  • 2 mm Gap Fill: Fills structural bond gaps up to 2 mm.
  • Extended Pot Life: Provides 40-60 minutes of usable life at 23 deg C.
  • FDA 175.105 Formulation: Specifically formulated to meet FDA 175.105 requirements.

Applications

Applications include structural bonding of metal, wood, composites, and certain plastics where controlled flow, gap filling, and FDA 175.105 adhesive positioning are required.

Product Family

PERMABOND ET5147

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Other Properties
Storage Temperature
5 to 25 °C
General Properties
Appearance
White / Ivory
Component System
Two (Epoxy Resin / Polyamine Hardener)
Mix Ratio
2:1 by volume
Pot Life
40-60 minutes
Specific Gravity
1.3 / 1.2
Thermal Properties
Glass Transition Temperature (Tg)
50-60 °C
Electrical Properties
Dielectric Strength
15-25 kV/mm

Additional Information

Technical properties

As supplied / before processing

Part A and Part B values are shown separately; processing values apply after the stated 2:1 mix ratio.

Property Value Unit Method / condition
AppearancePart A: white; Part B: ivoryAs supplied
Part A viscosity25,000-40,000mPa s20 rpm at 25 deg C
Part B viscosity90,000-150,000mPa s20 rpm at 25 deg C
Specific gravityPart A: 1.3; Part B: 1.2As supplied
Mix ratio2:1By volume
Maximum gap fill2mmTypical curing property
Usable / pot life40-60minutes2+1 g at 23 deg C
Handling time3-5hoursAt 23 deg C
Technical properties

After processing / final state

Property Value Unit Method / condition
Shear strength - mild steel18-20N/mm2ISO 4587
Shear strength - stainless steel15-19N/mm2ISO 4587
Shear strength - aluminum10-14N/mm2ISO 4587
Peel strength - aluminum40-70N/25 mmISO 4578
Hardness68-72Shore DISO 868
Glass transition temperature, Tg50-60deg CTypical cured value
Dielectric strength15-25kV/mmTypical cured value