PERMABOND ET502

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

PERMABOND ET502

Main features

  • Clear Two-Part Epoxy Bondline
  • 5-10 Minute Handling Strength
  • 4 mm Gap Filling

Product Description

Permabond ET502 is a colorless two-part epoxy adhesive for general-purpose bonding where a clear bondline and room-temperature cure are required. The 1:1 system has a mixed viscosity of 45,000-90,000 mPa s at 25 deg C, fills gaps up to 4 mm, and provides a 3-5 minute pot life at 23 deg C. Handling strength is reached in 5-10 minutes, with full cure after 24 hours at 23 deg C. Applications include wood, metals, ceramics, selected plastics, and composites.

Key features

  • Clear Bondline: Colorless components cure to a clear epoxy bondline.
  • Rapid Handling: Reaches handling strength in 5-10 minutes at 23 deg C.
  • 4 mm Gap Fill: Fills bond gaps up to 4 mm with a 1:1 mix ratio.

Applications

Applications include general-purpose bonding of wood, metals, ceramics, selected plastics, and composites where a clear bondline is required.

Product Family

PERMABOND ET502

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Colorless
Component System
Two (Epoxy Resin / Amine Hardener)
Mix Ratio
1:1 by volume
Pot Life
3-5 minutes
Specific Gravity
1.2 / 1.1
Other Properties
Maximum gap fill
4 mm
Mechanical Properties
Elongation
<5 %
Peel Strength
5-20 N/25mm
Thermal Properties
Glass Transition Temperature (Tg)
40-50 °C
Electrical Properties
Dielectric Strength
15-25 kV/mm

Additional Information

Technical properties

As supplied / before processing

Part A and Part B values are shown separately; mixed values apply after the stated 1:1 ratio.

Property Value Unit Method / condition
AppearancePart A: colorless; Part B: colorlessAs supplied
Part A viscosity80,000-150,000mPa sAt 25 deg C
Part B viscosity10,000-25,000mPa sAt 25 deg C
Mixed viscosity45,000-90,000mPa sAt 25 deg C
Specific gravityPart A: 1.2; Part B: 1.1As supplied
Mix ratio1:1By volume
Maximum gap fill4mmTypical curing property
Usable / pot life3-5minutesAt 23 deg C
Technical properties

After processing / final state

Property Value Unit Method / condition
Shear strength - mild steel8-12N/mm2ISO 4587
Peel strength - aluminum5-20N/25 mmISO 4578
Hardness70-80Shore DISO 868
Elongation at break<5%ISO 37
Glass transition temperature, Tg40-50deg CTypical cured value
Dielectric strength15-25kV/mmTypical cured value