PERMABOND ET-5428

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

PERMABOND ET-5428

Main features

  • 5 mm Composite Gap Filling
  • 30-45 Minute Handling Strength
  • High Shear and Peel Strength

Product Description

Permabond ET5428 is a two-part thixotropic epoxy adhesive formulated for tough, high-strength composite assembly bonding. Its controlled-flow consistency fills gaps up to 5 mm, while the 2:1 mix ratio and 10-20 minute pot life at 23 deg C support measured mixing or cartridge dispensing. Handling strength is reached in 30-45 minutes, and full cure develops in 24-48 hours at 23 deg C or 1 hour at 60 deg C. Typical cured performance includes 28-34 N/mm2 shear strength on mild steel and 150-250 N/25 mm peel strength on aluminum.

Key features

  • Composite Assembly Bonding: Formulated for tough, high-strength bonding of composite assemblies.
  • 5 mm Gap Fill: Controlled-flow thixotropy fills gaps up to 5 mm.
  • Rapid Handling: Reaches handling strength in 30-45 minutes at 23 deg C.

Applications

Applications include structural bonding of composite assemblies and gap-filling epoxy bonds that require controlled flow, high shear strength, and high peel strength.

Product Family

PERMABOND ET-5428

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
White / Cream
Component System
Two (Epoxy Resin / Polyamine Hardener)
Mix Ratio
2:1 by weight
Specific Gravity
1.1
Other Properties
Maximum gap fill
5 mm
Mechanical Properties
Elongation
<5 %
Thermal Properties
Glass Transition Temperature (Tg)
50-60 °C
Electrical Properties
Dielectric Strength
15-25 kV/mm

Additional Information

Technical properties

As supplied / before processing

Part A and Part B values are shown separately; processing values apply after the stated 2:1 mix ratio.

Property Value Unit Method / condition
Part A viscosity115,000mPa s20 rpm at 25 deg C
Part B viscosity200,000mPa s20 rpm at 25 deg C
Specific gravityPart A: 1.1; Part B: 1.1As supplied
Mix ratio2:1By volume and by weight
Maximum gap fill5mmTypical curing property
Usable / pot life10-20minutes10 g mixed at 23 deg C
Handling time30-45minutesAt 23 deg C
Full cure24-48 hours; 1 hourAt 23 deg C; at 60 deg C
Technical properties

After processing / final state

Property Value Unit Method / condition
Shear strength - mild steel28-34N/mm2ISO 4587
Shear strength - aluminum22-28N/mm2ISO 4587
Shear strength - stainless steel29-35N/mm2ISO 4587
Peel strength - aluminum150-250N/25 mmISO 4578
Impact strength30-40kJ/m2ASTM D-950
Hardness65-75Shore DISO 868
Glass transition temperature, Tg50-60deg CTypical cured value