PERMABOND ES550

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PERMABOND ES550

Main features

  • Toughened Structural Bonding
  • High-Viscosity Placement Control
  • No-Mix Bonding Processing

Product Description

Permabond® ES550 is a single-part, heat-curing epoxy paste designed for applications requiring high-performance structural bonds. Formulated to be slump-resistant, it will not flow during the heat-curing process, ensuring precise application. This toughened epoxy delivers exceptional shear, peel, and impact strength, making it highly effective for bonding a wide range of materials, including metals, ferrites, ceramics, and composites.

Key features

  • Toughened for high strength: Delivers outstanding impact resistance, alongside excellent shear and peel strength.
  • Slump-resistant paste: The extremely high viscosity (1,000,000 to 2,000,000 cP) paste formulation ensures the adhesive will not flow during the elevated temperatures required for curing.
  • Single-part convenience: Requires no mixing and cures rapidly with heat, eliminating the risk of mixing errors and improving production efficiency.

Applications / Suitable for

  • Bonding metals, ferrites, ceramics, and composites
  • Applications requiring a non-sagging adhesive during heat cure
  • Structural assemblies subject to high impact and vibration
Product Family

PERMABOND ES550

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Silver-grey
Solids
100 %
Specific Gravity
1.5
Physical Properties
Viscosity
1,000,000 to 2,000,000 mPa.s
Mechanical Properties
Elongation
>3 %
Impact Strength
25-35 KJ/m² mm
Peel Strength
43.75 N
Thermal Properties
Glass Transition Temperature (Tg)
120 °C
Thermal Conductivity
0.55 W/m.K
Other Properties
Maximum gap fill
5 mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Epoxy Resin - -
Appearance Silver-grey - Paste
Viscosity 1,000,000 to 2,000,000 cP at 25°C (Helipath, 2rpm) (mPa.s)
Specific Gravity 1.5 - -
Maximum Gap Fill 5 mm (0.2 in)
Flash Point > 100 °C (212°F)
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Cure Speed < 3 minutes Induction
Cure Speed 75 minutes Oven at 130°C (266°F)
Cure Speed 60 minutes Oven at 150°C (300°F)
Cure Speed 40 minutes Oven at 170°C (338°F)
Shear Strength 27-41 N/mm² Steel (ISO 4587) (4000-6000 psi)
Shear Strength > 14 N/mm² Steel to ferrite (>2000 psi) Substrate failure
Impact Strength 25-35 KJ/m² ASTM D-950
Hardness 80-85 Shore D ISO 868
E-modulus 4.8 GPa -
Elongation at Break < 3 % DIN 53504
Coefficient of Thermal Expansion 45E-6 mm/m/°C (below Tg)
Coefficient of Thermal Expansion 160E-6 mm/m/°C (above Tg)
Thermal Conductivity 0.55 W/(m.K) -
Glass Transition Temperature (Tg) 120 °C (250°F) DSC