PERMABOND 940

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND 940

Main features

  • Non-Frosting Alkoxyethyl Formulation
  • Low-Odor Cyanoacrylate Bonding
  • Fast Multi-Substrate Fixturing

Product Description

Permabond® 940 Cyanoacrylate is a low-odor, non-frosting, alkoxyethyl-based cyanoacrylate adhesive engineered to improve worker comfort and maintain a clean aesthetic. This 100% reactive, single-component adhesive cures rapidly at room temperature, eliminating the unsightly white fogging (blooming) that commonly occurs with standard cyanoacrylates on hot and humid days. It is surface-insensitive and rapidly bonds a wide range of materials, including plastics, metals, elastomers, and acidic surfaces.

Key features

  • Low odor formulation: Alkoxyethyl chemistry significantly reduces irritating fumes, improving worker comfort during application.
  • Non-frosting/Non-fogging: Eliminates the white residue (blooming) adjacent to the bondline, ensuring a flawless aesthetic appearance on finished parts.
  • Fast room-temperature cure: Provides rapid fixture times (e.g., 2-5 seconds on Neoprene/NBR and 10-15 seconds on steel), eliminating the need for mixing or heat.

Applications / Suitable for

  • Applications requiring a clean, fog-free aesthetic finish
  • Environments where low-odor adhesives are necessary for worker comfort
  • Rapid bonding of plastics, metals, and elastomers
Product Family

PERMABOND 940

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Liquid
Chemistry Type
Alkoxyethyl cyanoacrylate
Color
Colourless
Specific Gravity
1.1
Physical Properties
Viscosity
3-10 mPa.s mPa.s
Mechanical Properties
Impact Strength
3-5 kJ/m² mm
Thermal Properties
Linear thermal expansion
90 x 10^-6 mm/mm/°C
Thermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric Strength
25 kV/mm
Maximum gap fill
0.05 mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Alkoxyethyl cyanoacrylate - -
Appearance Colorless - Liquid
Viscosity 3-10 cP at 25°C (mPa.s)
Specific Gravity 1.1 - -
Maximum Gap Fill 0.05 mm (0.002 in)
Flash Point 80-93 °C (176°F - 199.94°F)
Volatile Organic Compound < 2 % 20 g/L (Estimated)
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Fixture/Handling Time 10-15 seconds Steel, Aluminium, PVC, Phenolic resin, ABS
Full Strength 24 hours -
Shear Strength 16-20 N/mm² Steel (ISO 4587) (2300-2900 psi)
Impact Strength 3-5 kJ/m² ASTM D-950 (1.4-2.4 ft-lb/in²)
Hardness 85 Shore D ISO 868
Dielectric Constant 3 - DIN 53483 at 1MHz
Dielectric Strength 25 kV/mm DIN 53481
Coefficient of Thermal Expansion 90E-6 mm/mm/°C -
Coefficient of Thermal Conductivity 0.1 W/(m.K) -