PERMABOND 919

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND 919

Main features

  • Up to 250 deg C Service
  • 20-Second Fixturing Time
  • MIL-A-46050C Type V Class 1 Approval

Product Description

Permabond® 919 Cyanoacrylate is an allyl-based, low-viscosity adhesive specifically engineered to meet high-temperature resistance requirements. While it cures rapidly at room temperature like traditional cyanoacrylates, it features a unique secondary curing mechanism activated by heat. Following a post-curing schedule, this 100% reactive, solvent-free adhesive can withstand extreme environmental temperatures up to 250°C (482°F).

Key features

  • Extreme temperature resistance: Secondary thermal cure mechanism allows the bonded joint to resist temperatures up to 250°C (482°F).
  • Fast setting: Delivers fixture handling times of under 20 seconds on steel, phenolic, and rubber substrates at room temperature.
  • Low viscosity: The 2-6 cP viscosity is ideal for tight-fitting parts and post-assembly wicking with a maximum gap fill of 0.05 mm.

Applications / Suitable for

  • Assemblies exposed to high-temperature environments (up to 250°C after post-cure)
  • Bonding metals (steel, aluminum), plastics, and rubbers
  • Military and aerospace applications requiring MIL-A-46050C Type V Class 1 approval
Product Family

PERMABOND 919

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Liquid
Chemistry Type
Allyl cyanoacrylate
Color
Colourless
Specific Gravity
1.1
Physical Properties
Viscosity
2-6 mPa.s
Mechanical Properties
Impact Strength
3-5 kJ/m² mm
Thermal Properties
Linear thermal expansion
90 x 10^-6 mm/mm/°C
Thermal Conductivity
0.1 W/m.K
Electrical Properties
Maximum gap fill
0.05 mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Allyl cyanoacrylate - -
Appearance Colorless - Liquid
Viscosity 2-6 cP at 25°C (mPa.s)
Specific Gravity 1.1 - -
Maximum Gap Fill 0.05 mm (0.002 in)
Flash Point 83 °C (181.4°F)
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Fixture/Handling Time < 20 seconds Steel, Buna N Rubber, Phenolic
Full Strength 24 hours -
Shear Strength 20-22 N/mm² Steel (ISO 4587) (2900-3200 psi)
Impact Strength 3-5 kJ/m² ASTM D-950 (1.4-2.4 ft-lb/in²)
Hardness 85 Shore D ISO 868
Coefficient of Thermal Expansion 90E-6 mm/mm/°C -
Coefficient of Thermal Conductivity 0.1 W/(m.K) -
Post-Cured Temperature Resistance 250 °C (482°F) after thermal activation