PERMABOND 795

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND 795

Main features

  • Moderate-Viscosity Surface-Insensitive Adhesive
  • 0.18 mm Maximum Gap Fill
  • MIL-A-46050C/CID A-A-3097 Compliance

Product Description

Permabond® 795 Cyanoacrylate is a moderate-viscosity, surface-insensitive adhesive designed to rapidly bond a wide variety of substrates, including difficult acidic surfaces like wood and plated metals. This 100% reactive, solvent-free formulation minimizes frosting and fogging during cure, making it ideal for clean, high-speed production lines. It reliably bonds plastics, metals, ceramics, and elastomers, achieving handling strength in just seconds without the need for mixing or heat curing.

Key features

  • Extremely fast setting: Polymerizes rapidly upon contact with surface moisture, delivering fixture handling times of approximately 4 seconds on steel, rubber, and phenolic.
  • Surface insensitive: Expertly engineered to form high-strength bonds on typically challenging acidic surfaces, such as wood and plated materials.
  • Industry approved: Meets stringent military and commercial specifications, including MIL-A-46050C Type II Class 3 (existing designs) and CID A-A-3097 Type II Class 3 (new designs).

Applications / Suitable for

  • Bonding acidic surfaces such as wood and plated surfaces
  • Adhering plastics, metals, ceramics, and elastomers
  • High-speed production lines requiring fast curing and moderate gap filling
Product Family

PERMABOND 795

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Liquid
Chemistry Type
Ethyl cyanoacrylate
Color
Colourless
Specific Gravity
1.1
Physical Properties
Viscosity
500 mPa.s mPa.s
Mechanical Properties
Impact Strength
3-5 kJ/m² mm
Thermal Properties
Thermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric Strength
25 kV/mm
Maximum gap fill
0.18 mm

Additional Information

Permabond® 795 Cyanoacrylate is a moderate-viscosity, surface-insensitive adhesive designed to rapidly bond a wide variety of substrates, including difficult acidic surfaces like wood and plated metals. This 100% reactive, solvent-free formulation minimizes frosting and fogging during cure, making it ideal for clean, high-speed production lines. It reliably bonds plastics, metals, ceramics, and elastomers, achieving handling strength in just seconds without the need for mixing or heat curing.

Key features

  • Extremely fast setting: Polymerizes rapidly upon contact with surface moisture, delivering fixture handling times of approximately 4 seconds on steel, rubber, and phenolic.
  • Surface insensitive: Expertly engineered to form high-strength bonds on typically challenging acidic surfaces, such as wood and plated materials.
  • Industry approved: Meets stringent military and commercial specifications, including MIL-A-46050C Type II Class 3 (existing designs) and CID A-A-3097 Type II Class 3 (new designs).

Applications / Suitable for

  • Bonding acidic surfaces such as wood and plated surfaces
  • Adhering plastics, metals, ceramics, and elastomers
  • High-speed production lines requiring fast curing and moderate gap filling
Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Ethyl cyanoacrylate - -
Appearance Colorless / Clear - Liquid
Viscosity 500 cP at 25°C (mPa.s)
Specific Gravity 1.1 - at 25°C
Maximum Gap Fill 0.18 mm (0.007 in)
Flash Point 80-93 °C (176°F - 199.94°F)
Volatile Organic Compound < 2 % 20 g/L (Estimated)
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Fixture/Handling Time 4 seconds Steel, Buna N Rubber, Phenolic
Full Strength 24 hours -
Shear Strength 18-22 N/mm² Steel (ISO 4587) (2600-3200 psi)
Impact Strength 3-5 kJ/m² ASTM D-950 (1.4-2.4 ft-lb/in²)
Hardness 85 Shore D ISO 868
Dielectric Constant 2.5 - at 10kHz
Dielectric Strength 25 kV/mm -
Coefficient of Thermal Expansion 90E-6 mm/mm/°C -
Coefficient of Thermal Conductivity 0.1 W/(m.K) -

Leading Brands Trust in Our Products and Services