PERMABOND 792

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND 792

Main features

  • Fast Surface-Insensitive Acidic-Substrate Bonding
  • 2 to 3-Second Fixture Time
  • MIL-A-46050C/NSF S4 Compliance

Product Description

Permabond® 792 Cyanoacrylate is a low-viscosity, surface-insensitive ethyl cyanoacrylate adhesive engineered for extremely fast setting. It is designed to rapidly bond a wide variety of materials, including plastics, metals, ceramics, elastomers, and difficult acidic substrates such as wood and plated surfaces. This 100% reactive, solvent-free formula minimizes frosting and fogging during cure and holds multiple industry approvals, including MIL-A-46050C and NSF.

Key features

  • Extremely fast setting: Achieves fixture handling times of just 2-3 seconds on steel, rubber, and phenolic surfaces, accelerating production.
  • Surface insensitive: Rapidly and reliably bonds challenging acidic substrates like wood and plated metals.
  • Industry approved: Meets MIL-A-46050C Type II Class 2, CID A-A-3097 Type II Class 2, and is NSF Approved (Non-food Compound Category Code S4).

Applications / Suitable for

  • Bonding acidic surfaces such as wood and plated surfaces
  • Adhering plastics, metals, ceramics, and elastomers
  • High-speed production lines requiring fast curing and no mixing
Product Family

PERMABOND 792

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Liquid
Chemistry Type
Ethyl cyanoacrylate
Color
Colourless
Specific Gravity
1.1
Physical Properties
Viscosity
60-125 mPa.s mPa.s
Mechanical Properties
Impact Strength
3-5 kJ/m² mm
Thermal Properties
Thermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric Strength
25 kV/mm
Maximum gap fill
0.15 mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Ethyl cyanoacrylate - -
Appearance Colorless - Liquid
Viscosity 60-125 cP at 25°C (mPa.s)
Specific Gravity 1.1 - -
Maximum Gap Fill 0.15 mm (0.006 in)
Flash Point 83 °C -
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Fixture/Handling Time 2-3 seconds Steel, Buna N Rubber, Phenolic
Full Strength 24 hours -
Shear Strength 18-22 N/mm² Steel (ISO 4587)
Tensile Strength > 20 N/mm² (ISO 6922)
Hardness 85 Shore D (ISO 868)
Dielectric Strength 25 kV/mm -
Coefficient of Thermal Conductivity 0.1 W/(m.K) -