PERMABOND 790

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND 790

Main features

  • 2 to 3-Second Handling Time
  • Surface-Insensitive Acidic-Substrate Bonding
  • Low-Viscosity Wicking Post-Assembly Bonding

Product Description

Permabond® 790 Cyanoacrylate is an extremely fast-setting, low-viscosity, surface-insensitive adhesive designed to rapidly bond a wide variety of substrates. Its specialized formulation readily bonds acidic surfaces such as wood and plated metals, along with plastics, ceramics, and elastomers. Featuring a highly penetrative wicking viscosity, this 100% reactive, solvent-free adhesive is ideal for post-assembly applications and minimizes the occurrence of frosting and fogging during cure.

Key features

  • Extremely fast setting: Single-component formula polymerizes rapidly upon contact with surface moisture, delivering fixture handling times of 2-3 seconds on steel and rubber.
  • Surface insensitive: Expertly engineered to rapidly bond notoriously difficult acidic surfaces, including wood and plated materials.
  • Low wicking viscosity: The exceptionally low 2 cP viscosity enables superior wicking action, making it perfectly suited for post-assembly penetration and application.

Applications / Suitable for

  • Bonding acidic surfaces such as wood and plated materials
  • Adhering plastics, metals, ceramics, and elastomers
  • Post-assembly applications utilizing wicking penetration
Product Family

PERMABOND 790

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Liquid
Chemistry Type
Ethyl cyanoacrylate
Color
Colourless
Specific Gravity
1.1
Physical Properties
Viscosity
2 mPa.s mPa.s
Mechanical Properties
Impact Strength
3-5 kJ/m² mm
Thermal Properties
Thermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric Strength
25 kV/mm
Maximum gap fill
0.05 mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Ethyl cyanoacrylate - -
Appearance Colorless - -
Viscosity 2 cP at 25°C (mPa.s)
Specific Gravity 1.1 - -
Maximum Gap Fill 0.05 mm (0.002 in)
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Fixture/Handling Time 2-3 seconds Steel, Buna N Rubber, Phenolic
Full Strength 24 hours -
Shear Strength 18-22 N/mm² Steel (ISO 4587) (2600-3200 psi)
Impact Strength 3-5 kJ/m² ASTM D-950 (1.4-2.4 ft-lb/in²)
Hardness 85 Shore D ISO 868
Dielectric Constant 2.5 - at 10kHz
Dielectric Strength 25 kV/mm -

Leading Brands Trust in Our Products and Services