PERMABOND 46

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

PERMABOND 46

Main features

  • No-Mix Surface Activation
  • Two-Hour Assembly Window
  • Low-Viscosity Controlled Application

Product Description

Permabond Initiator 46 is an amber liquid initiator used as the activation component in compatible Permabond no-mix acrylic bonding systems. It is applied to one surface while the adhesive is applied to the mating surface, allowing the components to be assembled without premixing the two materials. In the TA4246 system, parts should be bonded immediately and within two hours after initiator application. The initiator has an approximate viscosity of 70 mPa s at 23 deg C and a relative density of 0.97. It functions as an initiator and is not a standalone adhesive.

Key features

  • No-Mix Activation: Applied separately from the compatible adhesive to eliminate premixing.
  • Two-Hour Assembly Window: TA4246 components may be bonded within two hours after initiator application.
  • Low-Viscosity Liquid: Approximate viscosity of 70 mPa s at 23 deg C supports thin application.

Applications

Applications include initiation of compatible Permabond no-mix acrylic bonding processes, including TA4246.

Product Family

PERMABOND 46

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Amber
Specific Gravity
0.96
Physical Properties
Viscosity
70 mPa.s
Thermal Properties
Flash Point
>140 °C
Other Properties
Storage Temperature
5 - 25 °C

Additional Information

Technical properties

As supplied / before processing

Physical values apply to the standalone initiator before application.

Property Value Unit Method / condition
Product formLiquidAs supplied
ColorAmberAs supplied
Relative density0.97As supplied
ViscosityApprox. 70mPa sAt 23 deg C
Initial boiling point162deg CAs supplied