PERMABOND 43

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

PERMABOND 43

Main features

  • 10 mPa s Low Viscosity
  • 30-Minute On-Part Life
  • Immediate No-Mix Assembly

Product Description

PERMABOND Initiator 43 is a green, solvent-free surface initiator for compatible PERMABOND TA structural acrylic adhesives used as no-mix resin-and-initiator systems. The 10 mPa s liquid is brushed, wiped, or sprayed as a thin, even coating on one mating surface, while adhesive is applied to the other. Parts can be assembled immediately without an evaporation wait, and the treated surface remains active for up to 30 minutes. Initiator 43 has a typical specific gravity of 1.0 and flash point above 90 deg C. Handling time after assembly depends on bond gap and the paired TA adhesive.

Key features

  • Immediate no-mix assembly: Coated parts can be mated without a solvent-evaporation waiting period.
  • Low-viscosity surface coating: A typical viscosity of 10 mPa s supports thin brush, wipe, or spray application.
  • Thirty-minute on-part life: The treated surface remains active for up to 30 minutes before assembly.

Applications / Suitable for

  • Initiating compatible PERMABOND TA structural acrylic adhesives
  • No-mix bonding with initiator on one surface and adhesive on the other
  • Immediate assembly after brush, wipe, or spray application
Product Family

PERMABOND 43

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Green
Specific Gravity
1.0
Physical Properties
Viscosity
10 mPa.s
Thermal Properties
Flash Point
>90 °C
Other Properties
Storage Temperature
5 - 25 °C

Additional Information

Technical properties

As-supplied and working properties

Property Value Unit Method / condition
Appearance Green liquid As supplied
Viscosity 10 mPa s Typical
Specific gravity 1.0 Typical
Flash point Greater than 90 deg C Typical
On-part life 30 min Treated surface
Shelf life 12 months Unopened; stored at 5-25 deg C