PERMABOND 41

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

PERMABOND 41

Main features

  • 30-Minute On-Part Life
  • Brush, Wipe, or Spray
  • No-Mix Acrylic Initiation

Product Description

PERMABOND Initiator 41 functions as an amber, solvent-free surface initiator for compatible PERMABOND TA structural acrylic adhesives in no-mix bonding systems. The liquid is applied in a thin film by brush, wipe, or spray to one mating surface, while the adhesive is applied to the other. Assembly begins when the parts are brought together, eliminating a separate resin-and-initiator mixing step. The treated surface remains active for up to 30 minutes. With a typical specific gravity of 1.0 and 90 deg C flash point, Initiator 41 requires a compatible TA adhesive to form the bond.

Key features

  • No-mix acrylic initiation: Activates compatible PERMABOND TA structural acrylic adhesives when coated parts are assembled.
  • Thirty-minute on-part life: The treated surface remains active for up to 30 minutes before mating.
  • Flexible application method: Supports brush, wipe, or spray application as a thin surface film.

Applications / Suitable for

  • Initiating compatible PERMABOND TA structural acrylic adhesives
  • No-mix bonding with initiator on one surface and adhesive on the other
  • Brush, wipe, or spray surface application
Product Family

PERMABOND 41

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Other Properties
Storage Temperature
5 - 25 °C
General Properties
Color
Amber
Physical Properties
Viscosity
<50 mPa.s
Thermal Properties
Flash Point
>90 °C

Additional Information

Technical properties

As-supplied and working properties

Property Value Unit Method / condition
Appearance Amber liquid As supplied
Specific gravity 1.0 Typical
Flash point 90 deg C Typical
On-part life 30 min Treated surface

Leading Brands Trust in Our Products and Services