Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PERMABOND 2K

Main features

  • 1 mPa s Low Viscosity
  • Eight-Hour Mixed Working Life
  • Visible Red Coverage

Product Description

PERMABOND 2K Primer is a two-component, red liquid surface treatment for preparing metal, glass, plastic, and composite substrates before bonding with engineering adhesives. The mixed primer has a typical viscosity of 1 mPa s and specific gravity of 1.0, allowing a thin, visible coating that indicates surface coverage. Its mixed working life is 8 hours, and unopened material has a 24-month shelf life when stored at 5-25 deg C. It is used before compatible epoxy, acrylic, polyurethane, and other engineering adhesive systems; the primer itself does not form the bonded joint.

Key features

  • Visible red coverage: The red liquid provides a visual indication of primer wetting and surface coverage.
  • Low-viscosity application: A typical viscosity of 1 mPa s supports thin surface treatment.
  • Eight-hour mixed life: The combined primer remains usable for up to 8 hours.

Applications / Suitable for

  • Preparing metal and glass surfaces before adhesive bonding
  • Preparing plastic and composite surfaces
  • Use before compatible epoxy, acrylic, and polyurethane adhesive systems
Product Family

PERMABOND 2K

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Other Properties
Storage Temperature
5 - 25 °C
General Properties
Color
Red
Component System
Two
Specific Gravity
1.0
Physical Properties
Viscosity
1 mPa.s
Thermal Properties
Flash Point
55 °C

Additional Information

Technical properties

As-supplied and working properties

Property Value Unit Method / condition
Appearance Red liquid Mixed primer
Viscosity 1 mPa s Typical
Specific gravity 1.0 Typical
Flash point 55 deg C Typical
Mixed working life 8 h After combining components
Shelf life 24 months Unopened; stored at 5-25 deg C