PERMABOND 240

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND 240

Main features

  • 15 to 20-Second Fixturing Time
  • Up to 0.4 mm Gap Filling
  • WRAS/MIL-A-46050C Qualification Scope

Product Description

Permabond® 240 Cyanoacrylate is a high-viscosity, single-component adhesive designed for large gap applications and bonding porous substrates. This 100% reactive formulation polymerizes rapidly at room temperature when pressed into a thin film, eliminating the need for mixing or heat curing. It is highly versatile, providing fast-setting, high-strength bonds on a wide variety of materials including plastics, rubbers, and metals.

Key features

  • Rapid, room-temperature cure: Achieves fixture handling times in just 15 to 20 seconds on materials like steel, Buna N rubber, and phenolic.
  • High viscosity: Optimized viscosity profile allows for a maximum gap fill of 0.4 mm (0.017 in) and makes it highly effective for porous substrates.
  • Industry approvals: Approved to MIL-A-46050C Type II Class 3 for existing designs and holds WRAS Drinking Water Approval.

Applications / Suitable for

  • Bonding plastics, rubbers, and metals
  • Large gap applications up to 0.4 mm
  • Porous substrates
Product Family

PERMABOND 240

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Liquid
Chemistry Type
Ethyl cyanoacrylate
Color
Colourless
Specific Gravity
1.1
Physical Properties
Viscosity
1,200-2,500 mPa.s mPa.s
Mechanical Properties
Impact Strength
3-5 kJ/m² mm
Thermal Properties
Thermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric Strength
25 kV/mm
Maximum gap fill
0.4 mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Ethyl cyanoacrylate - -
Appearance Colorless - -
Viscosity 1,200-2,500 cP at 25°C (mPa.s)
Specific Gravity 1.1 - -
Maximum Gap Fill 0.4 mm (0.017 in)
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Fixture/Handling Time 15-20 seconds Steel, Buna N Rubber, Phenolic
Full Strength 24 hours -
Shear Strength 21-25 N/mm² Steel (ISO 4587)
Shear Strength 8-9 N/mm² Aluminium (ISO 4587)
Impact Strength 3-5 kJ/m² ASTM D-950
Hardness 85 Shore D ISO 868
Dielectric Strength 25 kV/mm -

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers