PERMABOND 200

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND 200

Main features

  • 1,500 mPa s Application Viscosity
  • 15-Second Fixturing Time
  • 22 N/mm^2 Shear Strength

Product Description

PERMABOND® 200 Cyanoacrylate Adhesive is a high-viscosity, single-component ethyl cyanoacrylate adhesive developed for wire-tacking and general component-bonding applications. Its 1,500 mPa·s viscosity supports controlled placement and helps bridge gaps up to 0.38 mm. The adhesive is suitable for plastics, rubber, and metals and reaches typical handling strength in approximately 15 seconds on steel, Buna N rubber, and phenolic. Full strength develops in 24 hours. The solvent-free, 100% reactive formulation requires no mixing or heat cure and is suited to rapid industrial assembly.

Key features

  • High-viscosity formulation: A viscosity of 1,500 mPa·s supports controlled application, wire tacking, and gap filling up to 0.38 mm.
  • Fast fixture performance: Reaches typical handling strength in approximately 15 seconds on steel, Buna N rubber, and phenolic.
  • Simple one-part processing: Requires no mixing or heat cure and contains no solvent.

Applications / Suitable for

  • Wire-tacking applications
  • Bonding components with small gaps
  • High-speed industrial assembly
  • Bonding plastics, rubber, and metals
Product Family

PERMABOND 200

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Liquid
Chemistry Type
Ethyl cyanoacrylate
Color
Colourless
Specific Gravity
1.05
Physical Properties
Viscosity
1,500 mPa.s
Mechanical Properties
Impact Strength
3-7 kJ/m² mm
Electrical Properties
Dielectric Strength
10 kV/mm
Maximum gap fill
038 mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and curing properties. Values are guideline information and do not constitute product specifications.

Property Value Unit Method / condition
Chemical composition Ethyl cyanoacrylate — Single-component adhesive
Appearance Colorless liquid — As supplied
Viscosity 1,500 mPa·s At 25 °C; equivalent to cP
Specific gravity 1.05 — Typical uncured value
Maximum gap fill 0.38 mm Equivalent source value 0.015 in
Fixture time — steel 15 s Time to 0.3 N/mm² shear strength
Fixture time — Buna N rubber 15 s Time to 0.3 N/mm² shear strength
Fixture time — phenolic 15 s Time to 0.3 N/mm² shear strength
Full strength 24 h Typical full-strength development
Technical properties

After-processing / final-state properties

Typical cured performance values. Bond strength varies with substrate, surface preparation, joint gap, and curing conditions.

Property Value Unit Method / condition
Shear strength — steel 22 N/mm² ISO 4587; equivalent source value 3,200 psi
Shear strength — aluminum 8 N/mm² ISO 4587; equivalent source value 1,200 psi
Impact strength 3–7 kJ/m² ASTM D950
Hardness 85 Shore D ISO 868
Dielectric strength 250 V/mil Typical cured electrical property
Minimum exposure temperature -55 °C Depends on the bonded materials; equivalent source value -65 °F