PERMABOND 130UV

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND 130UV

Main features

  • Rapid UV Bonding Cure
  • 200 mPa s Application Viscosity
  • Under 405 Nm LED Conditions

Product Description

PERMABOND® 130UV Light Cure Cyanoacrylate Adhesive is a low-viscosity, solvent-free, dual-cure adhesive designed for rapid bonding of metals and plastics. It combines conventional moisture-initiated cyanoacrylate curing with UV-light curing, allowing exposed adhesive fillets to become tack-free in seconds while small shadowed areas continue to cure through ambient moisture. The adhesive is yellow before cure and becomes clear in a thin bondline. At 25 °C, its 200 mPa·s viscosity supports controlled dispensing, accurate alignment, and automated application. Depending on the substrate, moisture-cure fixture times range from approximately 3 to 80 seconds, while UV exposure at 405 nm can produce a tack-free surface in 1–5 seconds under the documented lamp conditions.

Key features

  • Dual-cure technology: UV light rapidly cures exposed fillets, while moisture curing supports polymerization in small shadow areas.
  • Fast tack-free performance: Achieves a tack-free surface in ≤1 second at 150 mW/cm² or ≤5 seconds at 25 mW/cm² using a 405 nm spot LED.
  • Reduced bloom and odor: Designed to minimize blooming and improve the finished appearance of transparent or exposed joints.

Applications / Suitable for

  • Bonding opaque substrates with exposed adhesive fillets
  • Bonding through transparent plastic components
  • Automated adhesive dispensing
  • Metal and plastic assembly
  • Applications requiring rapid UV cure with secondary shadow-area cure
Product Family

PERMABOND 130UV

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Liquid
Chemistry Type
Ethyl cyanoacrylate
Color
Yellow before cure Clear in a thin bondline
Specific Gravity
1.1
Physical Properties
Open time
3s minutes
Tack-Free Time
<1s minutes
Viscosity
200 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and curing properties. Values are guideline information and do not constitute product specifications.

Property Value Unit Method / condition
Chemical composition Ethyl cyanoacrylate — Single-component, dual-cure adhesive
Appearance Yellow before cure; clear in a thin bondline — Fluoresces under UV light
Viscosity 200 mPa·s At 25 °C; equivalent to cP
Specific gravity 1.1 — Typical uncured value
Moisture fixture time — NBR 3 s 22 °C and 50% relative humidity
Moisture fixture time — steel 30 s 22 °C and 50% relative humidity
Moisture fixture time — polycarbonate 40 s 22 °C and 50% relative humidity
UV tack-free time ≤1 s 405 nm spot LED at 150 mW/cm²
UV tack-free time ≤5 s 405 nm spot LED at 25 mW/cm²
Technical properties

After-processing / final-state properties

Typical cured performance values. Unless otherwise stated, shear values are based on a 24-hour moisture cure. Results vary with substrate, preparation, bondline, and UV exposure.

Property Value Unit Method / condition
Shear strength — abraded mild steel 12–17 N/mm² ISO 4587; 24-hour moisture cure; equivalent source range 1,740–2,465 psi
Shear strength — stainless steel 14–19 N/mm² ISO 4587; 24-hour moisture cure
Shear strength — aluminum 5–9 N/mm² ISO 4587; 24-hour moisture cure
Shear strength — polycarbonate 6–10 N/mm² ISO 4587; 24-hour moisture cure
Shear strength — PMMA 7–11 N/mm² ISO 4587; 24-hour moisture cure
Shear strength — PVC 8–12 N/mm² ISO 4587; 24-hour moisture cure
Hardness 70–80 Shore D ISO 868
Biocompatibility Cytotoxicity tested — ISO 10993-5; claim requires compliance review