PERMABOND 102

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND 102

Main features

  • Low 70–90 mPa·s viscosity
  • 0.15 mm maximum gap fill
  • Typical fixture times of 5–15 seconds

Product Description

PERMABOND® 102 Cyanoacrylate Adhesive is a low-viscosity, single-component ethyl cyanoacrylate adhesive designed for fast bonding of close-fitting components. According to the TDS, its 70–90 mPa·s viscosity supports controlled flow into small bond gaps while maintaining rapid fixture performance. It is suitable for plastics, rubber, and metals, with a maximum recommended gap fill of 0.15 mm. Depending on the substrate, handling strength is typically reached within 5–15 seconds, while full strength develops in approximately 24 hours. The cured adhesive provides high shear strength on metals and selected plastics together with electrical insulating properties suitable for general industrial assembly.

Key features

  • Low-viscosity formulation: A TDS viscosity of 70–90 mPa·s supports bonding of close-fitting components and narrow joints.
  • Fast fixture performance: Typical handling strength is achieved in approximately 5–15 seconds depending on substrate.
  • Multi-material bonding: Documented performance includes steel, aluminum, zinc, ABS, PVC, polycarbonate, phenolic, and Buna N rubber.

Applications / Suitable for

  • Close-fitting component assembly
  • Plastic and rubber bonding
  • Metal bonding
  • High-speed production and fast-fixturing applications
  • Small-gap joints up to 0.15 mm
Product Family

PERMABOND 102

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Liquid
Chemistry Type
Ethyl cyanoacrylate
Color
Colourless
Specific Gravity
1.1
Physical Properties
Viscosity
70-90 mPa.s
Curing Conditions
Fixture Time
10-15 seconds
Mechanical Properties
Impact Strength
3-5 kJ/m² mm
Thermal Properties
Linear thermal expansion
90 x 10^-6 mm/mm/°C
Thermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric Strength
25 kV/mm
Maximum gap fill
0.15 mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and curing properties from the product technical datasheet. Values are guideline information and do not constitute product specifications.

Property Value Unit Method / condition
Chemical composition Ethyl cyanoacrylate — Single-component adhesive
Appearance Colorless — As supplied
Viscosity 70–90 mPa·s At 25 °C; TDS value; equivalent to cP
Specific gravity 1.1 — Typical uncured value
Maximum gap fill 0.15 mm Equivalent source value 0.006 in
Fixture time — steel 10–15 s Time to 0.3 N/mm² shear strength
Fixture time — Buna N rubber 5–10 s Time to 0.3 N/mm² shear strength
Fixture time — phenolic 10–15 s Time to 0.3 N/mm² shear strength
Fixture time — PVC 7–10 s Time to 0.3 N/mm² shear strength
Fixture time — ABS 7–10 s Time to 0.3 N/mm² shear strength
Full strength 24 h Typical full-strength development
Technical properties


After-processing / final-state properties

Typical cured performance values from the TDS. Bond strength varies with substrate, surface preparation, bond gap, and curing conditions.

Property Value Unit Method / condition
Shear strength — steel 19–23 N/mm² ISO 4587; equivalent source range 2,800–3,300 psi
Shear strength — aluminum 7–9 N/mm² ISO 4587; equivalent source range 1,000–1,300 psi
Shear strength — zinc 8–10 N/mm² ISO 4587; equivalent source range 1,200–1,500 psi
Shear strength — ABS >6 N/mm² ISO 4587; substrate failure reported
Shear strength — PVC >6 N/mm² ISO 4587; substrate failure reported
Shear strength — polycarbonate >5 N/mm² ISO 4587; substrate failure reported
Shear strength — phenolic 12–14 N/mm² ISO 4587; equivalent source range 1,700–2,000 psi
Impact strength 3–5 kJ/m² ASTM D950
Hardness 85 Shore D ISO 868
Dielectric constant 2.5 — At 10 kHz
Dielectric strength 25 kV/mm Typical cured electrical property
Coefficient of thermal expansion 90 × 10-6 mm/mm/°C Typical cured thermal property
Thermal conductivity 0.1 W/(m·K) Typical cured thermal property
Minimum exposure temperature -55 °C Depends on bonded materials; equivalent source value -65 °F

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers