PERMABOND 101

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND 101

Main features

  • 2 to 3 mPa s Viscosity Range
  • 2 to 10-Second Fixturing Time
  • 25 kV/mm Dielectric Strength

Product Description

PERMABOND® 101 Cyanoacrylate Adhesive is an ultra-low-viscosity, single-component ethyl cyanoacrylate adhesive for wicking into close-fitting joints and bonding pre-assembled parts. It cures rapidly when confined as a thin film between surfaces, with typical handling strength reached in 2–10 seconds depending on the substrate. The adhesive is suitable for plastics, rubber, and metals and has a maximum recommended gap fill of 0.05 mm. After cure, it provides high shear strength on steel and other substrates, 85 Shore D hardness, and electrical insulation properties suitable for industrial assembly applications.

Key features

  • Ultra-low viscosity: A 2–3 mPa·s viscosity supports capillary wicking into closely fitted and pre-assembled joints.
  • Fast fixture time: Typical handling strength is achieved in 2–10 seconds, depending on the bonded substrate.
  • Multi-material bonding: Supports bonding of plastics, rubber, and metals, with documented shear data on steel, aluminum, zinc, ABS, PVC, polycarbonate, and phenolic.

Applications / Suitable for

  • Pre-assembled components
  • Close-fitting plastic parts
  • Wicking and penetrating applications
  • High-speed industrial assembly
  • Bonding plastics, rubber, and metals
Product Family

PERMABOND 101

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Liquid
Chemistry Type
Ethyl cyanoacrylate
Color
Colourless
Specific Gravity
1.1
Physical Properties
Viscosity
2-3 mPa.s
Mechanical Properties
Impact Strength
3-5 kJ/m² mm
Thermal Properties
Thermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric Strength
25 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and curing properties. Values are guideline information and are not product specifications.

Property Value Unit Method / condition
Chemical composition Ethyl cyanoacrylate — Single-component adhesive
Appearance Colorless liquid — As supplied
Viscosity 2–3 mPa·s At 25 °C; equivalent to cP
Specific gravity 1.1 — Typical uncured value
Maximum gap fill 0.05 mm Equivalent source value 0.002 in
Fixture time — steel 3–5 s Time to 0.3 N/mm² shear strength
Fixture time — Buna N rubber 2–5 s Time to 0.3 N/mm² shear strength
Full strength 24 h Typical full-strength development
Technical properties

As-supplied / before-processing properties

Typical uncured and curing properties. Values are guideline information and are not product specifications.

Property Value Unit Method / condition
Chemical composition Ethyl cyanoacrylate — Single-component adhesive
Appearance Colorless liquid — As supplied
Viscosity 2–3 mPa·s At 25 °C; equivalent to cP
Specific gravity 1.1 — Typical uncured value
Maximum gap fill 0.05 mm Equivalent source value 0.002 in
Fixture time — steel 3–5 s Time to 0.3 N/mm² shear strength
Fixture time — Buna N rubber 2–5 s Time to 0.3 N/mm² shear strength
Full strength 24 h Typical full-strength development