OPTOLINQ WMC-1100| White Mold Compound

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

OPTOLINQ WMC-1100| White Mold Compound

Main features

  • White
  • High reflectance
  • Excellent reliability

Product Description

OPTOLINQ WMC-1100 is a white epoxy molding compound specifically designed for the encapsulation of optoelectronic devices. With its high spiral flow, WMC-1100 exhibits outstanding moldability, which allows for precise and intricate molding of optoelectronic devices and ensures consistent and high-quality production. This on top of its high thermal resistance and excellent reliability make WMC-1100 an ideal choice for optoelectronic device encapsulation.

Product Family

OPTOLINQ WMC-1100

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
White
Specific Gravity
2.1
Physical Properties
Spiral Flow @ 175°C
70-160 cm
Thermal Properties
Glass Transition Temperature (Tg)
150 °C
Curing Conditions
Transfer Pressure
10-30 kg/cm2
Transfer Time
40-100 s

Additional Information

Processing Instructions

  • Before use, allow WMC-1100 to reach room temperature for a minimum of 8 hours, ensuring the bag remains unopened to prevent moisture contamination.
  • Apply an outer releasing agent, such as silicones or fluorinated compounds, to the mold surface to facilitate easy release from the mold dies.
  • Prior to molding with WMC-1100 or any new material, the mold should be cleaned thoroughly. For proper mold conditioning, the initial three shots should be cured for 5–10 minutes. After this initial conditioning period, you can reduce the curing time to a level that provides sufficient hot hardness for effective release.

Storage and Handling

OPTOLINQ WMC-1100 is available in pressed pellets in a wide range of sizes to meet specific customer needs. To ensure product integrity, keep it away from oxidizing materials. For long-term storage, maintain a cold environment, ideally at –20 °C or lower. The shelf life under this condition is 12 months.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers