OPTOLINQ PM-1212 | Two-part silicone potting

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

OPTOLINQ PM-1212 | Two-part high power silicone potting

Main features

  • High optical transparency
  • Excellent UV and thermal resistance
  • Excellent adhesion to different materials

Product Description

OPTOLINQ PM-1212 is a premium two-part silicone potting material engineered for optoelectronic and high-power LED applications. This thermally stable, UV-resistant compound offers high optical transparency and exceptional long-term durability, making it an ideal choice for applications where light transmission, environmental resistance, and electrical insulation are critical.

The formulation features excellent adhesion to a wide variety of materials, making it suitable for diverse package configurations in automotive lighting, backlighting systems, and other precision electronics. Designed for shape control, reliability, and processability, PM-1212 is your go-to material when performance under harsh conditions is non-negotiable.

Product Family

OPTOLINQ PM-1212

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent
Mix Ratio
1:10
Pot Life
5 hours
Refractive index
1.41
Mechanical Properties
Elongation
45 %
Physical Properties
Viscosity
1100 mPa.s

Additional Information

Processing Instructions

  • Mix Parts A and B in a 1:10 weight ratio. Ensure that the mixture is uniform and free from streaks or unevenness.

  • Defoam the mixture under vacuum. 

  • Typical curing conditions: First cure at 60-80°C for 1 hour, followed by post cure at 150°C for 3h.

 

Precautions

  1. Addition-cure materials may be susceptible to inhibition by certain substances, including organotin and other organometallic compounds, silicone rubber with organotin catalyst, sulfur-containing materials such as polysulfones, amines, urethanes, amine-containing materials, unsaturated hydrocarbon plasticizers, and some solder flux residues. Always exercise caution and conduct thorough compatibility testing when encountering materials or chemicals of concern in your specific application to prevent potential curing issues.

  2. Avoid skin and eye contact. In case of contact, rinse thoroughly with soap (for skin) or clean water (for eyes), and seek medical attention if needed.

  3. Maintain a clean and ventilated workplace, using extraction trunks when necessary.

  4. Wear appropriate protective equipment and minimize direct contact with the human body. Refer to the Safety Data Sheet (SDS) before use.

 

Please note that the provided information is based on available data and typical conditions. For specific applications and detailed test results, refer to the actual test data and conduct appropriate certifications.

 

Cleaning

Uncured silicone can be easily removed using acetone or xylene. Polar solvents, including water and alcohols, are not recommended for cleaning.

 

Storage and Handling

Store in a ventilated, dry, and clean environment below 25°C. Do not allow moisture to come into contact with these materials. Containers should always remain tightly sealed. For partially filled containers, it is recommended to purge them with dry air or inert gases like nitrogen to maintain product integrity. At proper storage conditions, Part A and B have a shelf life of 6 months.

 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers