OPTOLINQ OLS-5812M | Liquid encapsulant - Two part silicone

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

OPTOLINQ OLS-5812M | Liquid encapsulant - Two part silicone

Main features

  • High reliability
  • Excellent thermal and light resistance
  • Excellent adhesion to different materials

Product Description

OPTOLINQ OLS-5812M is a two-part silicone encapsulant designed for the encapsulation of high-power LED products. Engineered with a focus on enhancing thermal stability, OLS-5812M contains fewer low molecular weight substances, considerably improving its heat resistance and adhesion strength. It also contains additives like antioxidants, which decrease the rate of thermo-oxidative aging and prolong the product's lifespan.

OLS-5812M offers good process compatibility. It is an ideal choice for industries seeking reliability, peak performance, and processability.

Product Family

OPTOLINQ OLS-5812M

1. Select Package Type
2. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Mix Ratio
1:4
Pot Life
4 hours
Refractive index
1.53
Thermal Properties
Temperature Resistance
-55 to 200 ˚C
Electrical Properties
Visible Light Transmission
>95 %
Physical Properties
Viscosity
2500 mPa.s

Additional Information

Processing Instructions

  • Mix Parts A and B in a 1:4 weight ratio. Ensure that the mixture is uniform and free from streaks or unevenness.
  • If air bubbles are entrapped during mixing, degas the mixture under vacuum.
  • Typical curing conditions:  First cure at 125 °C for 5 min, followed by post cure at 150 °C for 180 min.

Precautions

  • Addition-cure materials may be susceptible to inhibition by certain substances, including organotin and other organometallic compounds, silicone rubber with organotin catalyst, sulfur-containing materials such as polysulfones, amines, urethanes, amine-containing materials, unsaturated hydrocarbon plasticizers, and some solder flux residues. Always exercise caution and conduct thorough compatibility testing when encountering materials or chemicals of concern in your specific application to prevent potential curing issues.
  • Avoid skin and eye contact. In case of contact, rinse thoroughly with soap (for skin) or clean water (for eyes), and seek medical attention if needed.
  • Maintain a clean and ventilated workplace, using extraction trunks when necessary.
  • Wear appropriate protective equipment and minimize direct contact with the human body. Refer to the Material Safety Data Sheet (SDS) before use.

Cleaning

Uncured silicone can be easily removed using common hydrocarbon solvents, such as toluene and hexane. Polar solvents, including water and alcohols, are not recommended for this application.

Storage and Handling

Store in a ventilated, dry, and clean environment below 25°C. Do not allow moisture to come into contact with these materials. Containers should always remain tightly sealed. n the case of partially filled containers, it is recommended to purge them with dry air or inert gases like nitrogen to maintain product integrity. At proper storage conditions, Part A and B have a shelf life of 6 months.

 