OPTOLINQ LE-EP123 | One-Part Epoxy encapsulant

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

OPTOLINQ LE-EP123 | One-Part Epoxy encapsulant

Main features

  • Excellent thermal stability
  • Excellent UV stability
  • High light transmittance

Product Description

OPTOLINQ LE-EP123 is a high-performance, single-component epoxy resin that delivers exceptional optical clarity, robust bonding, and thermal stability. It's ideal for demanding applications where light transmission and structural integrity are critical.

OPTOLINQ LE-EP123 offers a wide curing temperature range, excellent anti-sagging properties, and superior high-temperature resistance, making it perfect for prepreg and impregnation processes. LE-EP123  is available with light diffusant depending on customer requirement.

Cure schedule

  • 150°C for 1 hour

 

Product Family

OPTOLINQ LE-EP123

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Colorless
Refractive index
1.52
Specific Gravity
1.00
Thermal Properties
Glass Transition Temperature (Tg)
115 °C
Electrical Properties
Visible Light Transmission
>90 %
Physical Properties
Viscosity
15000 mPa.s

Additional Information

...

OPTOLINQ LE-EP123 | Optically Clear Encapsulant

One part optically clear encapsulant. 

OPTOLINQ LE-EP123D | Light Diffusing Encapsulant

Optically clear encapsulation with diffusing capabilities.

LEEP123_OpticalPerformance
 

Precautions for Use

  1. This product needs to be stored at low temperatures and at dry places. The shelf life will vary depending on the storage conditions.

  2. Before use, allow the material to reach room temperature (15–25 °C, 25–55% RH) for at least 2 to 4 hours, ensuring the packaging is unopened to prevent moisture contamination—thawing time of approximately 2 hours for small packaging (30g). for larger quantities, it may take around 4 hours. 

  3. Preheat the material at 40-60°C for about  30-60 minutes

  4. Maintain a clean and ventilated workplace with proper ventilation and exhaust system..

  5. Wear appropriate safety equipment before use and avoid direct contact with the body. Please read the Safety Data Sheet (SDS) carefully before using.

  6. For standard applications using the single-step cure is sufficient and efficient. However for high-performance applications and thermally-sensitive packages and substrate please conduct specific tests to arrive at conditions suitable for the package.

 

Storage and Handling

Store in a cold, dry, and clean environment, ideally at –10 °C or lower with relative humidity below 70%. Keep away from exposure to direct sunlight. It is strictly forbidden to store in outdoor environments. At proper storage conditions, unopened material has a shelf life of 3 months.

 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers