OPTOLINQ LE-5031HY | Two part epoxy resin

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

OPTOLINQ LE-5031HY | Two part epoxy resin

Main features

  • Low viscosity
  • High transparency
  • Excellent solvent, aging, anti yellowing, and thermal resistance

Product Description

OPTOLINQ LE-5031HY is a low-viscosity, two-part, halogen-free epoxy resin with high transparency and a high-gloss finish. It offers robust stability in acidic and alkaline environments, good anti-aging properties, high durability even under extreme temperatures, and superior scratch and abrasion resistance. For specific color requirements, LE-5031HY can be customized using color or opaque pastes. The LE-5031HY is the anti-yellowing resistant version of LE-5031

OPTOLINQ LE-5031HY is a suitable coating for metal and polymer surfaces, providing a polished finish and excellent surface integrity. It is the preferred choice for coating solar cell panels, transparent potting of electronic components for insulation and moisture-proofing, high-voltage coil potting, and room temperature potting of capacitors and transformers. LE-5031HY complies with ROHS and REACH standards, offering a reliable solution for encapsulation and sealing applications.

Cure Schedule

  • 24h @ 25°C
  • 2-4h @ under 60C°
  • 1h @ 100°C
Product Family

OPTOLINQ LE-5031HY

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Mix Ratio
3:1
Pot Life
1 hours
Electrical Properties
Dielectric Strength
12–18 kV/mm
Surface Resistivity
>1.5×10¹⁵ Ohms/sq
Volume Resistivity
>1.6×10¹⁵ Ohms⋅cm
Mechanical Properties
Elongation
3.6 %
Chemical Properties
Water Absorption
0.15 %
Physical Properties
Viscosity
449 mPa.s

Additional Information

Anti-yellowing Performance


The following optical images of cured LE-5031HY samples (10 and 30 g) demonstrate its anti-yellowing capability under two distinct conditions: exposure to 70 °C for 18 hours and  to 85 °C at 85% RH for 24 hours.

Recommended Curing Conditions

Cure at 25 °C for 24 h or at 100 °C for 1 h.

These guidelines offer recommended curing parameters. Define the exact curing parameters to align with your product specifications.

Precautions for Use

  1. Follow the recommended mixing ratio (3:1) precisely.
  2. Make sure to stir the mixture thoroughly. Use the mixture as soon as possible.
  3. When the relative humidity >85%, the solid surface can absorb moisture from the air, producing a white fog. Room temperature curing is not advised when the relative humidity is greater than 85%. Instead, consider heated curing as a recommended alternative.
  4. After each use, seal the container tightly to prevent moisture from infiltrating and compromising the product's quality.

Storage and Handling

Store in a ventilated, dry, and clean environment. Keep away from fire and heat sources. It is strictly forbidden to store in outdoor environments. At proper storage conditions, Part A and Part B both have a shelf life of 180 days. Shelf life can be extended by using cold storage.

 