OPTOLINQ LE-2161HT | Two part BPA-free epoxy resin

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

OPTOLINQ LE-2161HT | Two part BPA-free epoxy resin

Main features

  • Low viscosity
  • Non-yellowing
  • High transparency and good mechanical properties

Product Description

OPTOLINQ LE-2161HT is a transparent, two-part BPA-free epoxy resin ideal for potting small components, sealing large dot matrix panels and wearable smart devices. It offers a fast curing rate, low curing temperature, and low viscosity post-mixing, and delivers exceptional electrical properties and anti-yellowing property upon curing. To meet specific color requirements, it can easily be colored and diffused using specialized dye concentrates and diffusant concentrates.

OPTOLINQ LE-2161HT serves as an ideal option for various electronic applications, including smart rings, due to its ability to encapsulate delicate electronic components while maintaining transparency and providing robust electrical insulation.

Key Features:

  • High Transmittance (Anti-Yellowing Performance)
  • BPA-Free, non-hazardous product (See SDS)
  • Low Viscosity and Good Wettability 
  • Excellent UV Resistance (QUV Aging Performance)

Highly Recommended For:

  • Wearable Smart Devices esp Smart Rings
  • Large Dot Matrix Panels
  • Small Consumer Electronics

Cure Schedule

  • 24h @ 25°C
  • 4h @ 50–60°C
  • 2h @ 80°C
Product Family

OPTOLINQ LE-2161HT

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Mix Ratio
3:1
Pot Life
1.5 hours
Electrical Properties
Dielectric Strength
16 kV/mm
Surface Resistivity
100000000000000 Ohms/sq
Visible Light Transmission
>90 %
Volume Resistivity
1000000000000000 Ohms⋅cm
Mechanical Properties
Elongation
4 %
Chemical Properties
Water Absorption
0.3 %
Physical Properties
Viscosity
370 mPa.s

Additional Information

 

Anti-yellowing Performance

The following optical images of cured LE-2161HT samples (1 and 2 mm) demonstrates its anti-yellowing capability under exposure to 70 °C for 24 hours at 90% RH.



LE-2161HTAnti-yellowing performance

QUV Aging Performance

The following optical images of cured LE-2161HT samples (1 and 2 mm) demonstrates QUV perrformance using standard QUV test: UV-A (340 nm), Irradiance: 0.76±0.02 W/m2 nm with specimen exposed to: 8H  drying, 0.25H water spray, 3.75H condensation and 50±3 °C black panel temperature.

LE-2161HTQUVagingperformance

 

Light Transmittance Data

 

LE-2161HTTransmittance

Precautions for Use

  1. The usable time after A and B are mixed strongly depends on the temperature and mixing volume. Higher temperatures and larger mixing volumes lead to shorter working times. Therefore, the mixing temperature and amount should be determined based on on-site procedures.
  2. Use the product in a clean and well-ventilated workplace.
  3. Wear appropriate safety equipment before use and avoid direct contact with the body. Please read the Safety Data Sheet (SDS) carefully before using.

 

 

Storage and Handling

Store in a ventilated, dry, and clean environment. Keep away from fire and heat sources. It is strictly forbidden to store in outdoor environments. The validity time will vary depending on storage conditions. At proper storage conditions, Part A and Part B have a shelf life of 183 and 183 days, respectively. Shelf life can be extended by using cold storage.

Note: Limited quantity exceptions  for LE-2161HT are 5L for passenger aircraft/rail and 60L for cargo aircraft. Under these quantities, LE-2161HT product benefit from reduced labeling requirements and need not be declared as dangerous goods.

 

Leading Brands Trust in Our Products and Services