MP 54190

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

MP 54190

Main features

  • 60-Minute Mixed Pot Life
  • Semi-Flexible 60% Elongation
  • 16.1 kV/mm Dielectric Strength

Product Description

H.B. Fuller MP54190 Epoxy Adhesive combines a mineral-filled two-part epoxy formulation with semi-flexible cured behavior for bonding metals and plastics. The translucent liquid components mix 1:1 by volume or 103:100 by weight and produce a typical mixed viscosity of 80,000 cP. A 100 g batch provides a 60-minute pot life at 25 deg C for cartridge or meter-mix-dispense application. Cure requires 48-72 hours at 23 deg C or 2 hours at 66 deg C. The cured epoxy reaches 60% elongation, 12.4 MPa overlap shear on acid-etched aluminum, and 16.1 kV/mm dielectric strength.

Key features

  • Sixty-minute pot life: A 100 g mixed mass provides a 60-minute working period at 25 deg C.
  • Semi-flexible cured epoxy: The cured material reaches 60% elongation with Shore D 70 hardness.
  • Electrical insulation data: The specified cured material has 16.1 kV/mm dielectric strength and a 4.5 dielectric constant at 100 Hz.

Applications / Suitable for

  • Metal assembly bonding
  • Plastic assembly bonding
  • Cartridge or meter-mix-dispense application
Product Family

MP 54190

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear
Chemistry Type
Epoxy
Component System
two component
Mechanical Properties
Elongation
60 %
Electrical Properties
Dielectric Strength
16.1 kV/mm
Volume Resistivity
8 E 13 Ohms⋅cm

Additional Information

Technical properties

Uncured and working properties

Property Value Unit Method / condition
Appearance Translucent liquid As supplied
Mix ratio 1:1 by volume; 103:100 by weight Resin to hardener
Mixed viscosity 80,000 cP Typical
Mixed specific gravity 1.32 Typical
Pot life 60 min 100 g mass at 25 deg C
Room-temperature cure 48-72 h 23 deg C
Heat cure 2 h 66 deg C
Technical properties

Cured properties

Property Value Unit Method / condition
Shore hardness 70 Shore D Cured adhesive
Operating temperature -60 to 150 deg C Typical range
Elongation 60 % Cured adhesive
Overlap shear 12.4 MPa ASTM D1002; acid-etched aluminum; 25 deg C; 50% RH
Tensile strength 20.7 MPa ASTM D638
Dielectric strength 16.1 kV/mm ASTM D149
Dielectric constant 4.5 ASTM D150; 25 deg C; 100 Hz