MOLYKOTE P-74

Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

MOLYKOTE P-74

Main features

  • Metal-Free Anti-Seize Formulation
  • 4,800 N Weld Load
  • Controlled M12 Fastener Friction

Product Description

MOLYKOTE P-74 Assembly Paste is a grayish-black, PAO-based, metal-free assembly paste with graphite and white solid lubricants for anti-seize and lubricating applications. The paste carries a typical 4,800 N four-ball weld load and has a service range of -40 to 200 deg C; selected raw materials continue to act as separating agents at 1,500 deg C in the dry-lubricant state. Applications include bolted connections, sliding bearings, linear guides, splined shafts, press-fit joints, exhaust and spark-plug threads, flanges, hinges, and brake mechanisms.

Key features

  • Metal-Free Anti-Seize Formulation: PAO base oil is combined with graphite and white solid lubricants without metallic solids.
  • 4,800 N Weld Load: The four-ball weld-load result is measured by DIN 51350, Part 4.
  • Controlled Fastener Friction: An M12 grade 8.8 test produced 0.14 thread and 0.08 head friction coefficients.

Applications / Suitable for

  • Bolted and threaded connections.
  • Sliding bearings, linear guides, and splined shafts.
  • Press-fit joints, flanges, hinges, and brake mechanisms.
  • Exhaust bolts and spark-plug threads.
Product Family

MOLYKOTE P-74

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Grayish black
Thermal Properties
Service temperature
as paste: -40 to 200 | as dry lubricant: 1500 °C

Additional Information

Technical properties

As-supplied paste properties

Property Value Unit Method / condition
Color Grayish black Typical
Physical form Paste Typical
Unworked penetration 280 to 310 mm/10 CTM 191; typical
Density 1.21 g/ml At 20 deg C; typical
Technical properties

In-service performance properties

Property Value Unit Method / condition
Paste service-temperature range -40 to 200 deg C Typical
Dry-lubricant separation function 1,500 deg C Selected raw materials continue to act as separating agents
Four-ball weld load 4,800 N DIN 51350, Part 4; typical
SRV oscillating wear duration 90 min 300 N, 1,000 um, 20 Hz at 90 deg C; typical
Thread/head friction coefficient 0.14 / 0.08 CTM 1153, M12 grade 8.8 blackened surface; typical
Press-fit friction coefficient 0.12 CTM 394; typical
Salt-spray duration 140 h ISO/R 1456 at 50 um coating thickness; typical
Emcor corrosion degree 2 DIN 51802; typical