MOLYKOTE P-3700

Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

MOLYKOTE P-3700

Main features

  • High-Purity Solid-Lubricant Paste
  • 3,000 N Weld Load
  • Controlled M12 Fastener Friction

Product Description

MOLYKOTE P-3700 Anti-Seize Paste is a dark-gray, high-purity mineral-oil paste with special solid lubricants for bolted joints exposed to elevated temperatures. The formulation contains no intentional calcium, lead, nickel, sulfur, chlorine, or fluorine and is suggested for high-chromium and stainless alloys. Typical data include a 3,000 N four-ball weld load, 280 to 320 unworked penetration, and controlled thread/head friction values for defined M12 fastener systems. The paste is applied to cleaned, fully coated screws, nuts, and bolts, while its solid lubricants resist temperatures from -30 to 900 deg C.

Key features

  • High-Purity Solid Lubricants: The formulation contains no intentional calcium, lead, nickel, sulfur, chlorine, or fluorine.
  • 3,000 N Weld Load: The four-ball weld-load result is measured by DIN 51350, Part 4.
  • Controlled Fastener Friction: M12 fastener tests provide thread, head, and K-factor values for blackened and stainless systems.

Applications / Suitable for

  • Screws, nuts, and bolts in elevated-temperature industrial equipment.
  • High-chromium alloy bolted joints.
  • Stainless-steel anti-seize applications.
Product Family

MOLYKOTE P-3700

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Dark Grey
Density (g)
1.23 g/cm3
Thermal Properties
Service temperature
-30 to +900 °C

Additional Information

Technical properties

As-supplied paste properties

Property Value Unit Method / condition
Appearance Dark gray Typical
Unworked penetration 280 to 320 mm/10 ISO 2137; typical
Density 1.23 g/cm3 ISO 2811 at 20 deg C; typical
Technical properties

In-service performance properties

Property Value Unit Method / condition
Service-temperature range -30 to 900 deg C Solid-lubricant paste; typical
Four-ball weld load 3,000 N DIN 51350, Part 4; typical
Four-ball wear scar 1.0 mm DIN 51350, Part 5 under 400 N load; typical
Thread/head friction coefficient 0.11 / 0.10 M12 x 1.75, grade 8.8, blackened surface; average
K-factor 0.14 M12 x 1.75, grade 8.8, blackened surface; average
Stainless thread/head friction coefficient 0.13 / 0.11 M12 x 1.75, A2-70, material 1.4301; average
Initial breakaway torque ~110 N m After 21 h at 540 deg C on material 1.7709; start torque 55 N m