MOLYKOTE P-1900

Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

MOLYKOTE P-1900

Main features

  • 3,200 N Weld Load
  • Controlled 0.10 Bolt Friction
  • -30 to 300 deg C Service

Product Description

MOLYKOTE P-1900 FM Anti-Seize Paste is a white mineral-oil/aluminum-complex anti-seize paste with solid lubricants for heavy-load mechanical contacts at low to medium speeds. It has NLGI 1 consistency, 34 mm2/s base-oil viscosity at 40 deg C, and a service range of -30 to 300 deg C. Typical performance data include a 3,200 N four-ball weld load and 0.10 thread and head friction coefficients on an M12 grade 8.8 bolted connection. The paste is applied to cleaned contact points by brush or grease gun for mechanical components in food and beverage processing equipment.

Key features

  • 3,200 N Weld Load: The four-ball weld-load result is measured by DIN 51350, Part 4.
  • Controlled Bolt Friction: Thread and head friction coefficients are both 0.10 on the M12 grade 8.8 test connection.
  • -30 to 300 deg C Service: The paste covers a broad operating-temperature range for mechanical contacts.

Applications / Suitable for

  • Mechanical components in food and beverage processing equipment.
  • Sliding surfaces under heavy loads.
  • Friction contacts operating at low to medium speeds.
Product Family

MOLYKOTE P-1900

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
White
Density (g)
1.0 to 1.04 g/cm3
Thermal Properties
Service temperature
-30 to +300 °C

Additional Information

Technical properties

As-supplied paste properties

Property Value Unit Method / condition
Color White Typical
NLGI consistency class 1 DIN 51818; typical
Unworked penetration 290 to 340 mm/10 Typical
Density 1.11 g/ml ISO 2811 at 20 deg C; typical
Base-oil viscosity 34 mm2/s DIN 51562 at 40 deg C; typical
Technical properties

In-service performance properties

Property Value Unit Method / condition
Service-temperature range -30 to 300 deg C Typical
Four-ball weld load 3,200 N DIN 51350, Part 4; typical
Four-ball wear scar 0.90 mm DIN 51350, Part 5 under 800 N load; typical
Thread/head friction coefficient 0.10 / 0.10 M12 grade 8.8 bolted connection; typical
Stainless thread/head friction coefficient 0.11 / 0.11 M12, material 1.4301; typical
Initial breakaway torque 85 N m After 21 h at 300 deg C on material 1.7709; starting torque 56 N m
Press-fit friction coefficient 0.10 Press-fit test; no chatter

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers