MOLYKOTE P-1042

Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

MOLYKOTE P-1042

Main features

  • 9,000 N Weld Load
  • Water-Emulsion Washout Resistance
  • High-Tack Metal Surface Adhesion

Product Description

MOLYKOTE P-1042 Adhesive Grease Paste is a light-beige, lithium-soap grease paste with mineral and synthetic oils, solid lubricants, and an adhesion improver for demanding metal-to-metal sliding contacts. The NLGI 1-2 paste carries a typical 9,000 N four-ball weld load and resists washout by water and metal-machining emulsions under the stated tests. Its paste service range is -25 to 120 deg C, while the solid-lubricant portion remains functional at 500 deg C. Application methods include brush, spatula, grease gun, automatic device, and central lubrication systems.

Key features

  • 9,000 N Weld Load: The four-ball weld-load result is measured by DIN 51350, Part 4.
  • Water-Emulsion Resistance: Static water resistance and washout tests support use around water and metal-machining emulsions.
  • High-Tack Metal Adhesion: The light-colored grease paste contains an adhesion improver for retention on metallic contact surfaces.

Applications / Suitable for

  • High-pressure metal-to-metal sliding surfaces.
  • Clamping tools exposed to water emulsions from metal machining.
  • Harsh contacts operating under combined load, temperature, or humidity.
Product Family

MOLYKOTE P-1042

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Light Beige
Density (g)
1.28 g/cm3
Thermal Properties
Service temperature
as paste: -25 to +120 | as lubricant: +500 °C

Additional Information

Technical properties

As-supplied paste properties

Property Value Unit Method / condition
Color Light beige Typical
NLGI class 1-2 DIN 51818; typical
Worked penetration 285 to 320 mm/10 ISO 2137; typical
Density 1.28 g/ml ISO 2811 at 20 deg C; typical
Drop point >150 deg C ISO 2176; test result, not a service-temperature limit
Technical properties

In-service performance properties

Property Value Unit Method / condition
Paste service-temperature range -25 to 120 deg C Typical
Solid-lubricant temperature 500 deg C Solid-lubricant state
Initial breakaway torque <300 x 10-3 N m ASTM D1478-80 at -20 deg C; typical
Running torque after 20 min <100 x 10-3 N m ASTM D1478-80 at -20 deg C; typical
Four-ball weld load 9,000 N DIN 51350, Part 4; typical
Four-ball wear scar 0.75 mm DIN 51350, Part 5 under 800 N load; typical
Water washout <5 wt% DIN 51807, Part 2 at 80 deg C for 1 h; typical
Emcor corrosion degree 0-1 DIN 51802; typical

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers