MOLYKOTE M-77

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE M-77

Main features

  • Up to 400 deg C Service
  • Silicone Carrier Oil
  • Selected Metal, Plastic, Rubber, and Elastomer Contacts

Product Description

MOLYKOTE® M-77 Paste is a black-gray solid-lubricant paste based on polyphenylmethyl siloxane oil, lithium soap, and molybdenum disulfide. It is intended for low-speed lubrication points operating under low to moderate loads, including applications exposed to water and extreme temperatures. The paste provides lubrication from −45°C to 230°C. Above 230°C, the silicone carrier volatilizes and the remaining dry lubricating film supports operation up to 400°C. The mineral-oil-free formulation is also suitable for selected elastomer and plastic components, subject to compatibility testing.

Key features

  • Wide temperature capability: Provides paste lubrication from −45°C to 230°C and dry-film lubrication up to 400°C.
  • Silicone carrier oil: Suitable for selected materials that are not resistant to mineral oils.
  • Solid-lubricant protection: Contains molybdenum disulfide to maintain lubrication after the carrier volatilizes.
  • Water resistance: Supports lubrication points exposed to water and moisture.
  • Low-speed performance: Formulated for low-speed contacts under low to moderate loads.
  • Flexible application: Can be applied by brush, spatula, grease gun, automatic lubricator, or compatible central lubrication system.

Applications / Suitable for

  • Metal-to-metal friction and contact surfaces
  • Plain bearings, bushings, and sleeves
  • Slides, guides, and tracks
  • Selected plastic, rubber, and elastomer components
  • Brake anchor plates and disc-brake pistons
  • Low-speed lubrication points exposed to water or extreme temperatures
Product Family

MOLYKOTE M-77

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product Type
Solid-lubricant paste; NLGI 2
Specific Gravity
1.95 g/mL at 20°C
Thermal Properties
Operating Temperature
−45°C to 230°C as paste; dry solid-lubricant film up to 400°C °C

Additional Information

MOLYKOTE® M-77 Paste is a black-gray solid-lubricant paste based on polyphenylmethyl siloxane oil, lithium soap, and molybdenum disulfide. It is intended for low-speed lubrication points operating under low to moderate loads, including applications exposed to water and extreme temperatures. The paste provides lubrication from −45°C to 230°C. Above 230°C, the silicone carrier volatilizes and the remaining dry lubricating film supports operation up to 400°C. The mineral-oil-free formulation is also suitable for selected elastomer and plastic components, subject to compatibility testing.

Key features

  • Wide temperature capability: Provides paste lubrication from −45°C to 230°C and dry-film lubrication up to 400°C.
  • Silicone carrier oil: Suitable for selected materials that are not resistant to mineral oils.
  • Solid-lubricant protection: Contains molybdenum disulfide to maintain lubrication after the carrier volatilizes.
  • Water resistance: Supports lubrication points exposed to water and moisture.
  • Low-speed performance: Formulated for low-speed contacts under low to moderate loads.
  • Flexible application: Can be applied by brush, spatula, grease gun, automatic lubricator, or compatible central lubrication system.

Applications / Suitable for

  • Metal-to-metal friction and contact surfaces
  • Plain bearings, bushings, and sleeves
  • Slides, guides, and tracks
  • Selected plastic, rubber, and elastomer components
  • Brake anchor plates and disc-brake pistons
  • Low-speed lubrication points exposed to water or extreme temperatures
Technical properties

After-application / in-service properties

Typical performance characteristics relevant to the applied paste and remaining dry lubricating film.

Property Value Unit Method / condition
Paste lubrication temperature range −45 to 230 °C Paste-like lubricating state
Dry-film temperature capability Up to 400 °C After carrier volatilization above 230°C
Four-ball weld load 2,000 N DIN 51350-4
Water resistance Good — Supplier-listed qualitative performance benefit
Carrier volatilization Leaves virtually no residue — At temperatures above 230°C; dry sliding film remains
Plastic and elastomer compatibility Compatible with many types — Compatibility testing required before use