MOLYKOTE HP-300

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE HP-300

Main features

  • Fully Fluorinated PFPE/PTFE Lubrication
  • 65 to 250 deg C Service Range
  • 3,300 N Four-Ball Weld Load

Product Description

MOLYKOTE® HP-300 Grease is a white, fully fluorinated lubricating grease based on perfluoropolyether oil with a PTFE thickener and PTFE solid lubricants. The NLGI Grade 2 formulation provides lubrication across a service-temperature range of −65°C to 250°C and resists chemicals, solvents, oxidation, and high-temperature exposure. It is suitable for harsh environments including corrosive service, liquefied natural gas, high vacuum, cleanroom equipment, and semiconductor manufacturing equipment where low lubricant volatilization is important. :contentReference[oaicite:0]{index=0}

Key features

  • Fully fluorinated formulation: Uses PFPE base oil with a PTFE thickener and PTFE solid lubricants.
  • Wide service-temperature range: Supports lubrication from −65°C to 250°C.
  • Chemical and solvent resistance: Formulated for harsh and chemically aggressive operating environments.
  • Low-volatility base oil: Provides a base-oil vapor pressure of 4 × 10−10 Pa at 20°C.
  • High-temperature stability: Shows 0.2% evaporation after 24 hours at 200°C under MIL-S-8660 testing.
  • Plastic compatibility: Compatible with most plastics.

Applications / Suitable for

  • Cleanroom and semiconductor manufacturing equipment
  • High-vacuum and low-volatilization applications
  • Corrosive and solvent-exposed equipment
  • Liquefied-natural-gas service
  • Rolling-element bearings, valves, packings, seals, and O-rings
  • Plastic, rubber, and elastomer lubrication
Product Family

MOLYKOTE HP-300

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product Type
Chemically resistant grease; NLGI 2
Specific Gravity
Approx. 1.9 g/mL at 20°C
Thermal Properties
Operating Temperature
−65°C to 300°C °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied characteristics and storage information for MOLYKOTE® HP-300 Grease. Values are not intended as specification limits. :contentReference[oaicite:1]{index=1}

Property Value Unit Method / condition
Technology Perfluoropolyether — PFPE-based grease
Thickener PTFE — Fluorinated-polymer thickener
Solid lubricant PTFE — Supplier-listed composition
Appearance White — Typical property
NLGI grade 2 — Consistency classification
Worked penetration, 60 strokes 280 0.1 mm JIS K 2220
Base-oil viscosity 160 cSt At 40°C
Density 2.0 g/cm³ Typical property
Usable life 36 months Unopened and stored in a cool, dark place
Technical properties

After-application / in-service properties

Typical performance characteristics relevant to the applied lubricant. Results apply only to the stated test methods and conditions. :contentReference[oaicite:2]{index=2}

Property Value Unit Method / condition
Service-temperature range −65 to 250 °C Supplier-listed service range
Bleed 8.0 % MIL-S-8660; 200°C for 24 hours
Evaporation 0.2 % MIL-S-8660; 200°C for 24 hours
Extended evaporation 1.0 % MIL-S-8660; 200°C for 1,000 hours
Four-ball weld load 3,300 N ASTM D2596; 1,500 rpm for 1 minute
Four-ball wear scar 1.1 mm ASTM D2266; 1,200 rpm, 392 N, 1 hour
Low-temperature torque 11 starting / 3.6 running N·cm JIS K 2220 at −40°C
Base-oil vapor pressure 4 × 10−10 Pa At 20°C