Main features

  • Plastic Gear Friction Control
  • 75 mm2/s Base Oil
  • Brush-to-Central System Application

Product Description

MOLYKOTE G-68 Plastic Gear Grease, 4 oz Tube is a 4 oz tube configuration of the mineral-oil/PAO G-68 plastic gear grease grade. The grease uses lithium soap, EP additives, and solid lubricants and has NLGI 2-3 consistency, 75 mm2/s base-oil viscosity at 40 deg C, and a -30 to 140 deg C service range. It can be applied by brush, spatula, grease gun, automatic device, or central lubrication system. Applications include electric toothbrush and paper-shredder gears and related plastic gear mechanisms using the G-68 grade.

Key features

  • Plastic Gear Friction Control: The G-68 grade produced a 0.014 steel-ball/POM friction coefficient under the specified test conditions.
  • 75 mm2/s Base Oil: The G-68 grade has 75 mm2/s base-oil viscosity at 40 deg C.
  • Flexible Grease Application: Supported methods include brush, spatula, grease gun, automatic device, and central lubrication system.

Applications / Suitable for

  • Gears in electric toothbrushes.
  • Gears in paper shredders.
  • Plastic gear mechanisms using the G-68 grade.
Product Family

MOLYKOTE G684OZTUBES

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
0.85 g/cm3
Thermal Properties
Service temperature
-30 to 140 °C

Additional Information

Technical properties

As-supplied grease properties

Technical values apply to the MOLYKOTE G-68 grease grade.

Property Value Unit Method / condition
NLGI consistency class 2-3 DIN 51818; G-68 grade, typical
Worked penetration 250 to 280 mm/10 ISO 2137; G-68 grade, typical
Density 0.85 g/ml ISO 2811 at 20 deg C; G-68 grade, typical
Base-oil viscosity 75 mm2/s DIN 51562 at 40 deg C; G-68 grade, typical
Drop point 190 deg C ISO 2176; G-68 grade, test result
Technical properties

In-service performance properties

Technical values apply to the MOLYKOTE G-68 grease grade.

Property Value Unit Method / condition
Service-temperature range -30 to 140 deg C G-68 grade, typical
Four-ball weld load 1,900 N DIN 51350, Part 4; G-68 grade, typical
Four-ball wear scar 0.75 mm DIN 51350, Part 5 under 600 N load; G-68 grade, typical
Almen-Wieland OK load 18,500 N G-68 grade, typical
Steel/POM friction coefficient 0.014 12.7 mm steel ball, 6.3 N, 10 mm/s, 24 h; G-68 grade, typical
Oil separation 3.4 % DIN 51817 / Federal Standard 791-32-2; G-68 grade, typical