MOLYKOTE G-N METAL ASSEMBLY PASTE

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE G-N METAL ASSEMBLY PASTE

Main features

  • Heavy-Duty Assembly Paste
  • 0.08 Coefficient of Friction
  • Metal Interfaces Protection

Product Description

MOLYKOTE® G-N Metal Assembly Paste is a multipurpose, heavy-duty lubricating paste containing molybdenum disulfide and white solid lubricants dispersed in mineral oil. Developed for metal surfaces subjected to extreme pressure and boundary-lubrication conditions, it provides a low coefficient of friction and helps reduce wear, galling, seizing and surface damage during assembly, running-in and maintenance. The paste also helps protect metal interfaces against fretting wear, corrosion and cold welding. It can be applied as a thin film to clean surfaces by burnishing with a lint-free cloth or brushing with short, stiff bristles.

Key features

  • Extreme-pressure lubrication: Lubricates metal surfaces under high-load and boundary-lubrication conditions, with a typical four-ball weld load of 499 kg (1,100 lb).
  • Low-friction performance: Provides a typical coefficient of friction of 0.08 in the CTM 0394 LFW-4 press-fit test.
  • Metal interface protection: Helps reduce galling, seizing, fretting wear, corrosion and cold welding during assembly, running-in and maintenance.

Applications / Suitable for

  • Running-in lubrication of gears, splines, journal bearings, cams and ways
  • Assembly and disassembly of threaded fasteners
  • Press fitting and interference fitting of metal components
  • Bearing shafts, bushings and splines exposed to fretting or cold welding
  • Metalworking operations including machining, stamping, drawing, tube bending, thread rolling, cold heading, swaging and forging
Product Family

MOLYKOTE G-N

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
buttery, grainy
Color
gray-black
Specific Gravity
1.33

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of MOLYKOTE® G-N Metal Assembly Paste in its as-supplied condition. Values are not intended for preparing specifications.

Property Value Unit Method / condition
Appearance Buttery, grainy paste — Typical
Color Gray–black — Typical
Consistency, penetration, unworked 300 mm/10 CTM 0300
Usable life 60 months From date of manufacture when stored at 32°F to 104°F (0°C to 40°C)
Technical properties

After-processing / final-state properties

Typical lubrication and in-use performance data. Values are not intended for preparing specifications and should not be used alone as the basis of design.

Property Value Unit Method / condition
Approximate service temperature range, solid lubricant 0 to 750 (-18 to 399) °F (°C) Solid-lubricant operating range
Approximate service temperature range, base oil 0 to 250 (-18 to 121) °F (°C) Base-oil operating range
Coefficient of friction 0.08 — CTM 0394; LFW-4 press-fit test, steel versus steel, velocity 0.6 in/min, 10,000 psi, room temperature
Four-ball wear scar 0.76 mm CTM 0351; 80 kg, 1 hour, 1,200 rpm, steel versus steel
Four-ball weld load 499 (1,100) kg (lb) Four-ball weld-load test
Effect on copper strip #1, no discoloration — CTM 0172; after 2 hours at 212°F (100°C)