MOLYKOTE® G-68 Plastic Gear Grease is an NLGI 2–3 lubricating grease formulated with mineral oil, polyalphaolefin, lithium soap, extreme-pressure additives and solid lubricants. Developed for plastic gearing, it combines good compatibility with most plastics, high water resistance and a low coefficient of friction. The grease operates across a documented service temperature range of -30 to +140°C and provides load-carrying and wear-protection performance for lubricated mechanical interfaces. Because plastic and elastomer formulations vary, compatibility testing is recommended before use.

Key features

  • Plastic compatibility: Provides good compatibility with most plastics; testing is recommended to evaluate swelling, shrinkage, stress cracking and changes in strength or hardness.
  • Low-friction lubrication: A coefficient of friction of 0.014 was measured between a steel ball and a POM surface under the documented test conditions.
  • Water-resistant performance: High water resistance supports lubrication in plastic gear mechanisms that may encounter moisture.

Applications / Suitable for

  • Plastic gears in electrical toothbrushes
  • Plastic gears in paper shredders
Product Family

MOLYKOTE G-68

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
0.85 g/cm3
Thermal Properties
Operating Temperature
-30 to +140 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the grease as supplied. These values are not intended for use as specification limits.

Property Value Unit Method / condition
NLGI consistency class 2–3 — DIN 51 818
Worked penetration 250–280 mm/10 ISO 2137
Density 0.85 g/ml ISO 2811; 20°C
Base oil viscosity 75 mm²/s DIN 51 562; 40°C
Drop point 190 °C ISO 2176
Technical properties

After-processing / final-state properties

Typical lubrication-performance values under the stated test conditions. These values are not intended for use as specification limits.

Property Value Unit Method / condition
Service temperature -30 to +140 °C Typical service range
Weld load 1,900 N DIN 51 350 T.4; four-ball tester (VKA)
Wear scar 0.75 mm DIN 51 350 T.5; four-ball tester, 600 N load
Almen-Wieland OK load 18,500 N Almen-Wieland machine
Coefficient of friction 0.014 μ Steel ball against POM; ball Ø 12.7 mm, load 6.3 N, speed 10 mm/s, 24 hours
Oxidation resistance 0.1 bar DIN 51 808; pressure drop after 100 hours at 99°C