MOLYKOTE D-321R AN-FR

Harmonization Code : 2710199990 |

MOLYKOTE D-321R AN-FR

Main features

  • Room-Temperature Application Cure
  • Dry Film Lubricant Formulation
  • 180 to 450 deg C Service Range

Product Description

MOLYKOTE® D-321 R Anti-Friction Coating is an air-curing dry-film lubricant supplied as a bulk liquid or aerosolized spray. Its solid-lubricant and binder system forms a gray-black lubricating film for high-load metal-to-metal interfaces operating with slow to medium-speed movement. The coating supports running-in and boundary-lubrication requirements while helping avoid stick-slip. A recommended dry-film thickness of 5 to 20 µm and a documented service temperature range of -180 to 450°C support evaluation across demanding mechanical assemblies and extreme-temperature environments.

Key features

  • Air-curing dry-film lubrication: Becomes touch-dry after 5 minutes at 23°C and is fully cured and ready for use after 2 hours at 23°C.
  • High-load metal interface performance: Formulated for metal-to-metal combinations with slow to medium-speed movement and high loads.
  • Broad service temperature range: The applied coating has a documented service temperature range of -180 to 450°C.

Applications / Suitable for

  • Plain bearings, bushings and sleeves
  • Power screw drives
  • Threaded connections and fasteners
  • Slides, guides and tracks
  • High-voltage switches, including operation under high vacuum and extreme temperatures
Product Family

MOLYKOTE D-321R AN-FR

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
gray-black
Density
1070 kg/m3
Thermal Properties
Operating Temperature
-180 - 450 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the bulk liquid coating. These values are not intended for use as specification limits.

Property Value Unit Method / condition
Color Gray-black — Typical
Viscosity 23 seconds ISO 2431; 23°C; #3 cup
Density 1.07 g/ml DIN 53217/2; 20°C
Nonvolatile content 29 % CTM 0242 I
Technical properties

After-processing / final-state properties

Typical dry-film performance values. Surface pretreatment codes are blank (b), phosphated (p) and sandblasted (s). These values are not specification limits.

Property Value Unit Method / condition
Service temperature range -180 to 450 °C Typical applied dry-film range
Falex load-carrying capacity b = 4,500; p = 12,500; s = 6,800 N ASTM D2625; results depend on surface pretreatment
LFW-I rotating service life to μ = 0.1 b = 212; p = 146; s = 306 revolutions × 1,000 ASTM D2714; F = 2,860 N; n = 72 rpm; V = 7.9 m/minute